Monolithic textured perovskite/silicon tandem solar cells(TSCs)are expected to achieve maximum light capture at the lowest cost,potentially exhibiting the best power conversion efficiency.However,it is challenging to ...Monolithic textured perovskite/silicon tandem solar cells(TSCs)are expected to achieve maximum light capture at the lowest cost,potentially exhibiting the best power conversion efficiency.However,it is challenging to fabricate high-quality perovskite films and preferred crystal orientation on commercially textured silicon substrates with micrometersize pyramids.Here,we introduced a bulky organic molecule(4-fluorobenzylamine hydroiodide(F-PMAI))as a perovskite additive.It is found that F-PMAI can retard the crystallization process of perovskite film through hydrogen bond interaction between F^(−)and FA^(+)and reduce(111)facet surface energy due to enhanced adsorption energy of F-PMAI on the(111)facet.Besides,the bulky molecular is extruded to the bottom and top of perovskite film after crystal growth,which can passivate interface defects through strong interaction between F-PMA+and undercoordinated Pb^(2+)/I^(−).As a result,the additive facilitates the formation of large perovskite grains and(111)preferred orientation with a reduced trap-state density,thereby promoting charge carrier transportation,and enhancing device performance and stability.The perovskite/silicon TSCs achieved a champion efficiency of 30.05%based on a silicon thin film tunneling junction.In addition,the devices exhibit excellent longterm thermal and light stability without encapsulation.This work provides an effective strategy for achieving efficient and stable TSCs.展开更多
Crystalline silicon(c-Si)heterojunction(HJT)solar cells are one of the promising technologies for next-generation industrial high-efficiency silicon solar cells,and many efforts in transferring this technology to high...Crystalline silicon(c-Si)heterojunction(HJT)solar cells are one of the promising technologies for next-generation industrial high-efficiency silicon solar cells,and many efforts in transferring this technology to high-volume manufacturing in the photovoltaic(PV)industry are currently ongoing.Metallization is of vital importance to the PV performance and long-term reliability of HJT solar cells.In this review,we summarize the development status of metallization approaches for highefficiency HJT solar cells.For conventional screen printing technology,to avoid the degradation of the passivation properties of the amorphous silicon layer,a low-temperature-cured(<250℃)paste and process are needed.This process,in turn,leads to high line/contact resistances and high paste costs.To improve the conductivity of electrodes and reduce the metallization cost,multi-busbar,fine-line printing,and low-temperature-cured silver-coated copper pastes have been developed.In addition,several potential metallization technologies for HJT solar cells,such as the Smart Wire Contacting Technology,pattern transfer printing,inkjet/FlexTrailprinting,and copper electroplating,are discussed in detail.B ased on the summary,the potential and challenges of these metallization technologies for HJT solar cells are analyzed.展开更多
Mono-crystalline silicon solar cells with a passivated emitter rear contact(PERC)configuration have attracted extensive attention from both industry and scientific communities.A record efficiency of 24.06%on p-type si...Mono-crystalline silicon solar cells with a passivated emitter rear contact(PERC)configuration have attracted extensive attention from both industry and scientific communities.A record efficiency of 24.06%on p-type silicon wafer and mass production efficiency around 22%have been demonstrated,mainly due to its superior rear side passivation.In this work,the PERC solar cells with a p-type silicon wafer were numerically studied in terms of the surface passivation,quality of silicon wafer and metal electrodes.A rational way to achieve a 24%mass-production efficiency was proposed.Free energy loss analyses were adopted to address the loss sources with respect to the limit efficiency of 29%,which provides a guideline for the design and manufacture of a high-efficiency PERC solar cell.展开更多
In order to enhance the p-type doping concentration in the LBSF, boron was added into the aluminum paste and boron doped local back surface field(B-LBSF) was successfully fabricated in this work. Through boron dopin...In order to enhance the p-type doping concentration in the LBSF, boron was added into the aluminum paste and boron doped local back surface field(B-LBSF) was successfully fabricated in this work. Through boron doping in the LBSF, much higher doping concentration was observed for the B-LBSF over the Al-LBSF. Higher doping concentration in the LBSF is expected to lead to better rear passivation and lower rear contact resistance. Based on one thousand pieces of solar cells for each type, it was found that the rear passivated crystalline silicon solar cells with B-LBSF showed statistical improvement in their photovoltaic properties over those with Al-LBSF.展开更多
Light trapping photonic crystal(PhC)patterns on the surface of Si solar cells provides a novel opportunity to approach the theoretical efficiency limit of 32.3%,for light-to-electrical power conversion with a single j...Light trapping photonic crystal(PhC)patterns on the surface of Si solar cells provides a novel opportunity to approach the theoretical efficiency limit of 32.3%,for light-to-electrical power conversion with a single junction cell.This is beyond the efficiency limit implied by the Lambertian limit of ray trapping~29%.The interference and slow light effects are harnessed for collecting light even at the long wavelengths near the Si band-gap.We compare two different methods for surface patterning,that can be extended to large area surface patterning:1)laser direct write and 2)step-&-repeat 5×reduction projection lithography.Large area throughput limitations of these methods are compared with the established elec-tron beam lithography(EBL)route,which is conventionally utilised but much slower than the presented methods.Spec-tral characterisation of the PhC light trapping is compared for samples fabricated by different methods.Reflectance of Si etched via laser patterned mask was~7%at visible wavelengths and was comparable with Si patterned via EBL made mask.The later pattern showed a stronger absorbance than the Lambertian limit6.展开更多
The ultraviolet(UV)light stability of silicon heterojunction(SHJ)solar cells should be addressed before large-scale production and applications.Introducing downshifting(DS)nanophosphors on top of solar cells that can ...The ultraviolet(UV)light stability of silicon heterojunction(SHJ)solar cells should be addressed before large-scale production and applications.Introducing downshifting(DS)nanophosphors on top of solar cells that can convert UV light to visible light may reduce UV-induced degradation(UVID)without sacrificing the power conversion efficiency(PCE).Herein,a novel composite DS nanomaterial composed of YVO_(4):Eu^(3+),Bi^(3+)nanoparticles(NPs)and AgNPs was synthesized and introduced onto the incident light side of industrial SHJ solar cells to achieve UV shielding.The YVO_(4):Eu^(3+),Bi^(3+)NPs and Ag NPs were synthesized via a sol-gel method and a wet chemical reduction method,respectively.Then,a composite structure of the YVO_(4):Eu^(3+),Bi^(3+)NPs decorated with Ag NPs was synthesized by an ultrasonic method.The emission intensities of the YVO_(4):Eu^(3+),Bi^(3+)nanophosphors were significantly enhanced upon decoration with an appropriate amount of~20 nm Ag NPs due to the localized surface plasmon resonance(LSPR)effect.Upon the introduction of LSPR-enhanced downshifting,the SHJ solar cells exhibited an~0.54%relative decrease in PCE degradation under UV irradiation with a cumulative dose of 45 k W h compared to their counterparts,suggesting excellent potential for application in UV-light stability enhancement of solar cells or modules.展开更多
In this work,we developed a simple and direct circuit model with a dual two-diode model that can be solved by a SPICE numerical simulation to comprehensively describe the monolithic perovskite/crystalline silicon(PVS/...In this work,we developed a simple and direct circuit model with a dual two-diode model that can be solved by a SPICE numerical simulation to comprehensively describe the monolithic perovskite/crystalline silicon(PVS/c-Si)tandem solar cells.We are able to reveal the effects of different efficiency-loss mechanisms based on the illuminated current density-voltage(J-V),semi-log dark J-V,and local ideality factor(m-V)curves.The effects of the individual efficiency-loss mechanism on the tandem cell’s efficiency are discussed,including the exp(V/VT)and exp(V/2VT)recombination,the whole cell’s and subcell’s shunts,and the Ohmic-contact or Schottky-contact of the intermediate junction.We can also fit a practical J-V curve and find a specific group of parameters by the trial-and-error method.Although the fitted parameters are not a unique solution,they are valuable clues for identifying the efficiency loss with the aid of the cell’s structure and experimental processes.This method can also serve as an open platform for analyzing other tandem solar cells by substituting the corresponding circuit models.In summary,we developed a simple and effective methodology to diagnose the efficiency-loss source of a monolithic PVS/c-Si tandem cell,which is helpful to researchers who wish to adopt the proper approaches to improve their solar cells.展开更多
The calculated and experimental research of sheet resistances of crystalline silicon solar cells by dry laser doping is investigated. The nonlinear numerical model on laser melting of crystalline silicon and liquid-ph...The calculated and experimental research of sheet resistances of crystalline silicon solar cells by dry laser doping is investigated. The nonlinear numerical model on laser melting of crystalline silicon and liquid-phase diffusion of phosphorus atoms by dry laser doping is analyzed by the finite difference method implemented in MATLAB. The melting period and melting depth of crystalline silicon as a function of laser energy density is achieved. The effective liquid-phase diffusion of phosphorus atoms in melting silicon by dry laser doping is confirmed by the rapid decrease of sheet resistances in experimental measurement. The plateau of sheet resistances is reached at around 15 Ω/. The calculated sheet resistances as a function of laser energy density is obtained and the calculated results are in good agreement with the corresponding experimental measurement. Due to the successful verification by comparison between experimental measurement and calculated results, the simulation results could be used to optimize the virtual laser doping parameters.展开更多
AIM: To investigate the expression differences of transforming growth factor-β2(TGF-β2), basic fibroblast growth factor(b FGF) and intercellular cell-adhesion molecule-1(ICAM-1) in lens epithelial cells(LECs...AIM: To investigate the expression differences of transforming growth factor-β2(TGF-β2), basic fibroblast growth factor(b FGF) and intercellular cell-adhesion molecule-1(ICAM-1) in lens epithelial cells(LECs) of complicated cataract with silicone oil tamponade and agerelated cataract. METHODS: Totally 150 eyes of 150 patients(aged 35 to 77y) were investigated, including 75 patients with complicated cataract after silicone oil tamponade and 75 patients with age-related cataract. The central piece of anterior capsules was collected during cataract surgery. TGF-β2, b FGF and ICAM-1 were detected in the 60 specimens of the two groups by immunohistochemistry. The expression levels of the three kinds of messenger ribonucleic acid(m RNA) were determined by real-time quantitative reverse transcriptionpolymerase chain reaction in the 90 specimens of the two groups.RESULTS: TGF-β2 was detected in the cytomembrane and cytoplasm of the LECs and b FGF was detected in the nucleus. ICAM-1 was positive in the cytomembrane of the LECs and the distribution of positive cells was uneven. The m RNA genes expression of the TGF-β2, b FGF and ICAM-1 was significant differences between the two groups and markedly increased in complicated cataract group(P〈0.05).CONCLUSION: The up-regulated TGF-β2, b FGF and ICAM-1 maybe associate with the occurrence and development of complicated cataract with silicone oil tamponade.展开更多
Finger interruptions are common problems in screen printed solar cells, resulting in poor performance in efficiency because of high effective series resistance. Electroluminescence(EL) imaging is typically used to i...Finger interruptions are common problems in screen printed solar cells, resulting in poor performance in efficiency because of high effective series resistance. Electroluminescence(EL) imaging is typically used to identify interrupted fingers. In this paper, we demonstrate an alternative method based on photoluminescence(PL) imaging to identify local series resistance defects, with a particular focus on finger interruptions. Ability to detect finger interruptions by using PL imaging under current extraction is analyzed and verified. The influences of external bias control and illumination intensity on PL images are then studied in detail. Finally, in comparison with EL imaging, the using of PL imaging to identify finger interruptions possesses the prominent advantages: in PL images, regions affected by interrupted fingers show higher luminescence intensity, while regions affected by recombination defects show lower luminescence intensity. This inverse signal contrast allows PL imaging to more accurately identify the defect types.展开更多
The detailed balance method is used to study the potential of the intermediate band solar cell (IBSC), which can improve the efficiency of the gi-based solar cell with a bandgap between 1.1 eV to 1.7 eV. It shows th...The detailed balance method is used to study the potential of the intermediate band solar cell (IBSC), which can improve the efficiency of the gi-based solar cell with a bandgap between 1.1 eV to 1.7 eV. It shows that a crystalline silicon solar ceil with an intermediate band located at 0.36 eV below the conduction band or above the valence band can reach a limiting efficiency of 54% at the maximum light concentration, improving greatly than 40.7% of the Shoekley-Queisser limit for the single junction Si solar cell. The simulation also shows that the limiting efficiency of the silicon-based solar cell increases as the bandgap increases from 1.1 eV to 1.7 eV, and the amorphous Si solar cell with a bandgap of 1.7 eV exhibits a radiative limiting efficiency of 62.47070, having a better potential.展开更多
Low energy hydrogen ion was used to passivate the electrically active defects existing in grains and grain boundaries of polycrystalline silicon solar cells.Short circuit current of H + implanted cells remarkably...Low energy hydrogen ion was used to passivate the electrically active defects existing in grains and grain boundaries of polycrystalline silicon solar cells.Short circuit current of H + implanted cells remarkably increased before and after preparing TiO 2AR(antireflective)coating.The measurements(at λ=6328) of the optical properties of H + implanted silicon samples show that:the value of absorption coefficient reached the level of a Si;refractive index n and reflectivity R significantly decreased;the optical band gap increased from 1.1 eV to 1.3 eV.The results indicate that Si H bonds have been formed after H + implantation.The calculation shows that the optical thickness cycle of TiO 2 AR coating will reduce correspondingly in order to obtain the optimum optical match between AR coating and implanted silicon since refractive index decreases after H + implantation.展开更多
A nano-structured surface is formed on the pyramid structure of n-type silicon solar cells by size-controlled silver nano-particle assisted etching. Such a nano-structure creates a front average weighted reflectance o...A nano-structured surface is formed on the pyramid structure of n-type silicon solar cells by size-controlled silver nano-particle assisted etching. Such a nano-structure creates a front average weighted reflectance of less than 2.5% in the 300-1200nm range due to the broadband reflection suppression. The sodium hydroxide is used to obtain the low-area surface by post-etching the nano-structure, thus the severe carrier recombination associated with the nano-structured surface could be reduced. After emitter forming, screen printing and firing by means of the industrial fabrication protocol, an 18.3%-efficient nano-structured silicon solar cell with rear emitter is fabricated. The process of fabricating the solar cells matches well with industrial manufacture and shows promising prospects.展开更多
Currently, 86% of the energy originates from fossil fuelsforelectricity. These are expected to run out, causing severe environmental damage threatening future generations. The total impact of Small and Medium Enterpri...Currently, 86% of the energy originates from fossil fuelsforelectricity. These are expected to run out, causing severe environmental damage threatening future generations. The total impact of Small and Medium Enterprises (SMEs) on the economy is significant. Solar cells harness the sun's energy to generate electricity in an environmentally friendly manner. This study compares silicon solar cells to flexible Organic Photovoltaic solar cells (OPV) for electricity energy for a micro-business in the UK and Iraq. It shows that it is feasible to replace existing fossil fuel sources with solar cells in Iraq due to a greater amount of solar radiation striking the earth's surface. Flexible solar cells can replace a proportion of the energy requirements in the UK and a larger proportion in Iraq. Using existing 20% efficient solar cells, 28% and 83% of the energy requirements of the microbusiness can be replaced in UK and Iraq respectively. Assuming 20% efficiency for solar cells placed on windows, 74% and 220% of the energy requirements of UK and Kurdistan can be replaced respectively and the surplus stored.展开更多
The silicon heterojunction(SHJ)solar cell has long been considered as one of the most promising candidates for the next-generation PV market.Transition metal oxides(TMOs)show good carrier selectivity when combined wit...The silicon heterojunction(SHJ)solar cell has long been considered as one of the most promising candidates for the next-generation PV market.Transition metal oxides(TMOs)show good carrier selectivity when combined with c-Si solar cells.This has led to the rapid demonstration of the remarkable potential of TMOs(especially MoO_(x))with high work function to replace the p-type a-Si:H emitting layer.MoO_(x) can induce a strong inversion layer on the interface of n-type c-Si,which is beneficial to the extraction and conduction of holes.In this paper,the radio-frequency(RF)magnetron sputtering is used to deposit MoO_(x) films.The optical,electrical and structural properties of MoO_(x) films are measured and analyzed,with focus on the inherent compositions and work function.Then the MoO_(x) films are applied into SHJ solar cells.When the MoO_(x) works as a buffer layer between ITO/p-a-Si:H interface in the reference SHJ solar cell,a conversion efficiency of 19.1%can be obtained.When the MoOx is used as a hole transport layer(HTL),the device indicates a desirable conversion efficiency of 17.5%.To the best of our knowledge,this current efficiency is the highest one for the MoO_(x) film as HTL by RF sputtering.展开更多
The laser equipment is one of the key equipment in the production line of the solar energy. In this article, the author de-scribes the application of the laser equipment in the production line of the amorphous silicon...The laser equipment is one of the key equipment in the production line of the solar energy. In this article, the author de-scribes the application of the laser equipment in the production line of the amorphous silicon film solar cells, and points out that the stable and exactitude is the key direction of the future development of the laser scribing equipment.展开更多
Silicon passivated emitter and rear contact(PERC) solar cells with V-groove texture were fabricated using maskless alkaline solution etching with in-house developed additive. Compared with the traditional pyramid text...Silicon passivated emitter and rear contact(PERC) solar cells with V-groove texture were fabricated using maskless alkaline solution etching with in-house developed additive. Compared with the traditional pyramid texture, the V-groove texture possesses superior effective minority carrier lifetime, enhanced p–n junction quality and better applied filling factor(FF). In addition, a V-groove texture can greatly reduce the shading area and edge damage of front Ag electrodes when the V-groove direction is parallel to the gridline electrodes. Due to these factors, the V-groove solar cells have a higher efficiency(21.78%) than pyramid solar cells(21.62%). Interestingly, external quantum efficiency(EQE) and reflectance of the V-groove solar cells exhibit a slight decrease when the incident light angle(θ) is increased from 0° to 75°, which confirms the excellent quasi omnidirectionality of the V-groove solar cells. The proposed V-groove solar cell design shows a 2.84% relative enhancement of energy output over traditional pyramid solar cells.展开更多
This article presents a three-dimensional analysis of the impact of the angle of incidence of the magnetic field intensity on the electrical performance (series resistance, shunt resistance) of a bifacial polycrystall...This article presents a three-dimensional analysis of the impact of the angle of incidence of the magnetic field intensity on the electrical performance (series resistance, shunt resistance) of a bifacial polycrystalline silicon solar cell. The cell is illuminated simultaneously from both sides. The continuity equation for the excess minority carriers is solved at the emitter and at the depth of the base respectively. The analytical expressions for photocurrent density, photovoltage, series resistance and shunt resistance were deduced. Using these expressions, the values of the series and shunt resistances were extracted for different values of the angle of incidence of the magnetic field intensity. The study shows that as the angle of incidence increases, the slopes of the minority carrier density for the two modes of operation of the solar cell decrease. This is explained by a drop in the accumulation of carriers in the area close to the junction due to the fact that the Lorentz force is unable to drive the carriers towards the lateral surfaces due to the weak action of the magnetic field, which tends to cancel out as the incidence angle increases, and consequently a drop in the open circuit photovoltage. This, in turn, reduces the Lorentz force. These results predict that the p-n junction of the solar cell will not heat up. The study also showed a decrease in series resistance as the incidence angle of the magnetic field intensity increased from 0 rad to π/2 rad and an increase in shunt resistance as the incidence angle increased. His behaviour of the electrical parameters when the angle of incidence of the field from 0 rad to π/2 rad shows that the decreasing magnetic field vector tends to be collinear with the electron trajectory. This allows them to cross the junction and participate in the external current. The best orientation for the Lorentz force is zero, in which case the carriers can move easily towards the junction.展开更多
By solving the magneto-transport equation for excess minority charge carriers in the base of the series vertical-junction silicon cell, the phenomenological parameters of the cell can be determined from the boundary c...By solving the magneto-transport equation for excess minority charge carriers in the base of the series vertical-junction silicon cell, the phenomenological parameters of the cell can be determined from the boundary conditions. Photocurrent density and photovoltage are determined for each value of applied magnetic field and corresponding optimum thickness, to establish the current-voltage characteristic (Jph(Sf, Sb, z, B, Hop)-Vph(Sf, Sb, z, B, Hop) of the silicon cell under polychromatic illumination. This study will make it possible to reduce the material used (by reducing the optimum thickness), which will help to lower prices. It will also enable us to reduce betting effects (lower series resistance), thereby boosting solar cell efficiency.展开更多
基金the financial support of National Key Research and Development Program of China(Grant No.2023YFB4202503)the Joint Funds of the National Natural Science Foundation of China(Grant No.U21A2072)+7 种基金Natural Science Foundation of China(Grant No.62274099)Natural Science Foundation of Tianjin(No.20JCQNJC02070)China Postdoctoral Science Foundation(No.2020T130317)the Overseas Expertise Introduction Project for Discipline Innovation of Higher Education of China(Grant No.B16027)Tianjin Science and Technology Project(Grant No.18ZXJMTG00220)Key R&D Program of Hebei Province(No.19214301D)provided by the Haihe Laboratory of Sustainable Chemical Transformationsthe Fundamental Research Funds for the Central Universities,Nankai University.
文摘Monolithic textured perovskite/silicon tandem solar cells(TSCs)are expected to achieve maximum light capture at the lowest cost,potentially exhibiting the best power conversion efficiency.However,it is challenging to fabricate high-quality perovskite films and preferred crystal orientation on commercially textured silicon substrates with micrometersize pyramids.Here,we introduced a bulky organic molecule(4-fluorobenzylamine hydroiodide(F-PMAI))as a perovskite additive.It is found that F-PMAI can retard the crystallization process of perovskite film through hydrogen bond interaction between F^(−)and FA^(+)and reduce(111)facet surface energy due to enhanced adsorption energy of F-PMAI on the(111)facet.Besides,the bulky molecular is extruded to the bottom and top of perovskite film after crystal growth,which can passivate interface defects through strong interaction between F-PMA+and undercoordinated Pb^(2+)/I^(−).As a result,the additive facilitates the formation of large perovskite grains and(111)preferred orientation with a reduced trap-state density,thereby promoting charge carrier transportation,and enhancing device performance and stability.The perovskite/silicon TSCs achieved a champion efficiency of 30.05%based on a silicon thin film tunneling junction.In addition,the devices exhibit excellent longterm thermal and light stability without encapsulation.This work provides an effective strategy for achieving efficient and stable TSCs.
基金supported by the Priority Academic Program Development of Jiangsu Higher Education Institutions(PAPD)。
文摘Crystalline silicon(c-Si)heterojunction(HJT)solar cells are one of the promising technologies for next-generation industrial high-efficiency silicon solar cells,and many efforts in transferring this technology to high-volume manufacturing in the photovoltaic(PV)industry are currently ongoing.Metallization is of vital importance to the PV performance and long-term reliability of HJT solar cells.In this review,we summarize the development status of metallization approaches for highefficiency HJT solar cells.For conventional screen printing technology,to avoid the degradation of the passivation properties of the amorphous silicon layer,a low-temperature-cured(<250℃)paste and process are needed.This process,in turn,leads to high line/contact resistances and high paste costs.To improve the conductivity of electrodes and reduce the metallization cost,multi-busbar,fine-line printing,and low-temperature-cured silver-coated copper pastes have been developed.In addition,several potential metallization technologies for HJT solar cells,such as the Smart Wire Contacting Technology,pattern transfer printing,inkjet/FlexTrailprinting,and copper electroplating,are discussed in detail.B ased on the summary,the potential and challenges of these metallization technologies for HJT solar cells are analyzed.
基金supported by the National Natural Science Foundation of China(No.61504155)。
文摘Mono-crystalline silicon solar cells with a passivated emitter rear contact(PERC)configuration have attracted extensive attention from both industry and scientific communities.A record efficiency of 24.06%on p-type silicon wafer and mass production efficiency around 22%have been demonstrated,mainly due to its superior rear side passivation.In this work,the PERC solar cells with a p-type silicon wafer were numerically studied in terms of the surface passivation,quality of silicon wafer and metal electrodes.A rational way to achieve a 24%mass-production efficiency was proposed.Free energy loss analyses were adopted to address the loss sources with respect to the limit efficiency of 29%,which provides a guideline for the design and manufacture of a high-efficiency PERC solar cell.
基金Funded by the National Natural Science Foundation of China(61366004)the Research Fund for the Doctoral Program of Higher Education(20123601110006)the Jiangxi Provincial Department of Education(KJLD13008)
文摘In order to enhance the p-type doping concentration in the LBSF, boron was added into the aluminum paste and boron doped local back surface field(B-LBSF) was successfully fabricated in this work. Through boron doping in the LBSF, much higher doping concentration was observed for the B-LBSF over the Al-LBSF. Higher doping concentration in the LBSF is expected to lead to better rear passivation and lower rear contact resistance. Based on one thousand pieces of solar cells for each type, it was found that the rear passivated crystalline silicon solar cells with B-LBSF showed statistical improvement in their photovoltaic properties over those with Al-LBSF.
基金project support by Nano-Processing Facility (NPF), AIST, Tsukuba, Japan where we were granted access to photo-lithography stepperARC DP190103284 "Photonic crystals: the key to breaking the silicon-solar cell efficiency barrier" project+1 种基金the visiting professor program at the Institute of Advanced Sciences at Yokohama National University (2018-20)Nanotechnology Ambassador fellowship at MCN (2012-19)
文摘Light trapping photonic crystal(PhC)patterns on the surface of Si solar cells provides a novel opportunity to approach the theoretical efficiency limit of 32.3%,for light-to-electrical power conversion with a single junction cell.This is beyond the efficiency limit implied by the Lambertian limit of ray trapping~29%.The interference and slow light effects are harnessed for collecting light even at the long wavelengths near the Si band-gap.We compare two different methods for surface patterning,that can be extended to large area surface patterning:1)laser direct write and 2)step-&-repeat 5×reduction projection lithography.Large area throughput limitations of these methods are compared with the established elec-tron beam lithography(EBL)route,which is conventionally utilised but much slower than the presented methods.Spec-tral characterisation of the PhC light trapping is compared for samples fabricated by different methods.Reflectance of Si etched via laser patterned mask was~7%at visible wavelengths and was comparable with Si patterned via EBL made mask.The later pattern showed a stronger absorbance than the Lambertian limit6.
基金supported by the National Natural Science Foundation of China (Grant Nos.52202276 and 51821002)the China Postdoctoral Science Foundation (Grant No.2022M712300)+1 种基金the Natural Science Foundation of the Jiangsu Higher Education Institutions of China (Grant No.22KJB480010)a project funded by the Priority Academic Program Development of Jiangsu Higher Education Institutions (PAPD)。
文摘The ultraviolet(UV)light stability of silicon heterojunction(SHJ)solar cells should be addressed before large-scale production and applications.Introducing downshifting(DS)nanophosphors on top of solar cells that can convert UV light to visible light may reduce UV-induced degradation(UVID)without sacrificing the power conversion efficiency(PCE).Herein,a novel composite DS nanomaterial composed of YVO_(4):Eu^(3+),Bi^(3+)nanoparticles(NPs)and AgNPs was synthesized and introduced onto the incident light side of industrial SHJ solar cells to achieve UV shielding.The YVO_(4):Eu^(3+),Bi^(3+)NPs and Ag NPs were synthesized via a sol-gel method and a wet chemical reduction method,respectively.Then,a composite structure of the YVO_(4):Eu^(3+),Bi^(3+)NPs decorated with Ag NPs was synthesized by an ultrasonic method.The emission intensities of the YVO_(4):Eu^(3+),Bi^(3+)nanophosphors were significantly enhanced upon decoration with an appropriate amount of~20 nm Ag NPs due to the localized surface plasmon resonance(LSPR)effect.Upon the introduction of LSPR-enhanced downshifting,the SHJ solar cells exhibited an~0.54%relative decrease in PCE degradation under UV irradiation with a cumulative dose of 45 k W h compared to their counterparts,suggesting excellent potential for application in UV-light stability enhancement of solar cells or modules.
基金This work was supported by Zhejiang Energy Group(znkj-2018-118)Key Research and Development Program of Zhejiang Province(2021C01006)+5 种基金Key Project of Zhejiang Province(2021C04009)Science and technology projects in Liaoning Province 2021(2021JH1/10400104)Ningbo“Innovation 2025”Major Project(2020Z098)National Key R&D Program of China(2018YFB1500403)National Natural Science Foundation of China(61974178,61874177,62004199)Youth Innovation Promotion Association(2018333).
文摘In this work,we developed a simple and direct circuit model with a dual two-diode model that can be solved by a SPICE numerical simulation to comprehensively describe the monolithic perovskite/crystalline silicon(PVS/c-Si)tandem solar cells.We are able to reveal the effects of different efficiency-loss mechanisms based on the illuminated current density-voltage(J-V),semi-log dark J-V,and local ideality factor(m-V)curves.The effects of the individual efficiency-loss mechanism on the tandem cell’s efficiency are discussed,including the exp(V/VT)and exp(V/2VT)recombination,the whole cell’s and subcell’s shunts,and the Ohmic-contact or Schottky-contact of the intermediate junction.We can also fit a practical J-V curve and find a specific group of parameters by the trial-and-error method.Although the fitted parameters are not a unique solution,they are valuable clues for identifying the efficiency loss with the aid of the cell’s structure and experimental processes.This method can also serve as an open platform for analyzing other tandem solar cells by substituting the corresponding circuit models.In summary,we developed a simple and effective methodology to diagnose the efficiency-loss source of a monolithic PVS/c-Si tandem cell,which is helpful to researchers who wish to adopt the proper approaches to improve their solar cells.
基金Supported by the National Natural Science Foundation of China under Grant No 61306076
文摘The calculated and experimental research of sheet resistances of crystalline silicon solar cells by dry laser doping is investigated. The nonlinear numerical model on laser melting of crystalline silicon and liquid-phase diffusion of phosphorus atoms by dry laser doping is analyzed by the finite difference method implemented in MATLAB. The melting period and melting depth of crystalline silicon as a function of laser energy density is achieved. The effective liquid-phase diffusion of phosphorus atoms in melting silicon by dry laser doping is confirmed by the rapid decrease of sheet resistances in experimental measurement. The plateau of sheet resistances is reached at around 15 Ω/. The calculated sheet resistances as a function of laser energy density is obtained and the calculated results are in good agreement with the corresponding experimental measurement. Due to the successful verification by comparison between experimental measurement and calculated results, the simulation results could be used to optimize the virtual laser doping parameters.
基金Supported by the Natural Science Foundation of Shaanxi Province(No.2012JM4023)
文摘AIM: To investigate the expression differences of transforming growth factor-β2(TGF-β2), basic fibroblast growth factor(b FGF) and intercellular cell-adhesion molecule-1(ICAM-1) in lens epithelial cells(LECs) of complicated cataract with silicone oil tamponade and agerelated cataract. METHODS: Totally 150 eyes of 150 patients(aged 35 to 77y) were investigated, including 75 patients with complicated cataract after silicone oil tamponade and 75 patients with age-related cataract. The central piece of anterior capsules was collected during cataract surgery. TGF-β2, b FGF and ICAM-1 were detected in the 60 specimens of the two groups by immunohistochemistry. The expression levels of the three kinds of messenger ribonucleic acid(m RNA) were determined by real-time quantitative reverse transcriptionpolymerase chain reaction in the 90 specimens of the two groups.RESULTS: TGF-β2 was detected in the cytomembrane and cytoplasm of the LECs and b FGF was detected in the nucleus. ICAM-1 was positive in the cytomembrane of the LECs and the distribution of positive cells was uneven. The m RNA genes expression of the TGF-β2, b FGF and ICAM-1 was significant differences between the two groups and markedly increased in complicated cataract group(P〈0.05).CONCLUSION: The up-regulated TGF-β2, b FGF and ICAM-1 maybe associate with the occurrence and development of complicated cataract with silicone oil tamponade.
基金supported by the National Natural Science Foundation of China(Grant Nos.61504139 and 61275040)the Fund from the Chinese Academy of Sciences(Grant No.Y072051002)
文摘Finger interruptions are common problems in screen printed solar cells, resulting in poor performance in efficiency because of high effective series resistance. Electroluminescence(EL) imaging is typically used to identify interrupted fingers. In this paper, we demonstrate an alternative method based on photoluminescence(PL) imaging to identify local series resistance defects, with a particular focus on finger interruptions. Ability to detect finger interruptions by using PL imaging under current extraction is analyzed and verified. The influences of external bias control and illumination intensity on PL images are then studied in detail. Finally, in comparison with EL imaging, the using of PL imaging to identify finger interruptions possesses the prominent advantages: in PL images, regions affected by interrupted fingers show higher luminescence intensity, while regions affected by recombination defects show lower luminescence intensity. This inverse signal contrast allows PL imaging to more accurately identify the defect types.
基金Project supported by the National Basic Research Program of China (Grant No.2007 CB613404)the National Natural Science Foundation of China (Grant Nos.61036001,60906035,and 51072194)
文摘The detailed balance method is used to study the potential of the intermediate band solar cell (IBSC), which can improve the efficiency of the gi-based solar cell with a bandgap between 1.1 eV to 1.7 eV. It shows that a crystalline silicon solar ceil with an intermediate band located at 0.36 eV below the conduction band or above the valence band can reach a limiting efficiency of 54% at the maximum light concentration, improving greatly than 40.7% of the Shoekley-Queisser limit for the single junction Si solar cell. The simulation also shows that the limiting efficiency of the silicon-based solar cell increases as the bandgap increases from 1.1 eV to 1.7 eV, and the amorphous Si solar cell with a bandgap of 1.7 eV exhibits a radiative limiting efficiency of 62.47070, having a better potential.
文摘Low energy hydrogen ion was used to passivate the electrically active defects existing in grains and grain boundaries of polycrystalline silicon solar cells.Short circuit current of H + implanted cells remarkably increased before and after preparing TiO 2AR(antireflective)coating.The measurements(at λ=6328) of the optical properties of H + implanted silicon samples show that:the value of absorption coefficient reached the level of a Si;refractive index n and reflectivity R significantly decreased;the optical band gap increased from 1.1 eV to 1.3 eV.The results indicate that Si H bonds have been formed after H + implantation.The calculation shows that the optical thickness cycle of TiO 2 AR coating will reduce correspondingly in order to obtain the optimum optical match between AR coating and implanted silicon since refractive index decreases after H + implantation.
基金Supported by the National Natural Science Foundation of China under Grant No 51532007the Major Projects of Zhejiang Province under Grant No 2013C01037the Foundation of State Key Lab of Silicon Materials
文摘A nano-structured surface is formed on the pyramid structure of n-type silicon solar cells by size-controlled silver nano-particle assisted etching. Such a nano-structure creates a front average weighted reflectance of less than 2.5% in the 300-1200nm range due to the broadband reflection suppression. The sodium hydroxide is used to obtain the low-area surface by post-etching the nano-structure, thus the severe carrier recombination associated with the nano-structured surface could be reduced. After emitter forming, screen printing and firing by means of the industrial fabrication protocol, an 18.3%-efficient nano-structured silicon solar cell with rear emitter is fabricated. The process of fabricating the solar cells matches well with industrial manufacture and shows promising prospects.
文摘Currently, 86% of the energy originates from fossil fuelsforelectricity. These are expected to run out, causing severe environmental damage threatening future generations. The total impact of Small and Medium Enterprises (SMEs) on the economy is significant. Solar cells harness the sun's energy to generate electricity in an environmentally friendly manner. This study compares silicon solar cells to flexible Organic Photovoltaic solar cells (OPV) for electricity energy for a micro-business in the UK and Iraq. It shows that it is feasible to replace existing fossil fuel sources with solar cells in Iraq due to a greater amount of solar radiation striking the earth's surface. Flexible solar cells can replace a proportion of the energy requirements in the UK and a larger proportion in Iraq. Using existing 20% efficient solar cells, 28% and 83% of the energy requirements of the microbusiness can be replaced in UK and Iraq respectively. Assuming 20% efficiency for solar cells placed on windows, 74% and 220% of the energy requirements of UK and Kurdistan can be replaced respectively and the surplus stored.
基金Project supported by the National Natural Science Foundation of China(Grant No.62074084)the National Key Research and Development Program of China(Grant No.2018YFB1500402)Key Research and Development Program of Hebei Province,China(Grant No.20314303D).
文摘The silicon heterojunction(SHJ)solar cell has long been considered as one of the most promising candidates for the next-generation PV market.Transition metal oxides(TMOs)show good carrier selectivity when combined with c-Si solar cells.This has led to the rapid demonstration of the remarkable potential of TMOs(especially MoO_(x))with high work function to replace the p-type a-Si:H emitting layer.MoO_(x) can induce a strong inversion layer on the interface of n-type c-Si,which is beneficial to the extraction and conduction of holes.In this paper,the radio-frequency(RF)magnetron sputtering is used to deposit MoO_(x) films.The optical,electrical and structural properties of MoO_(x) films are measured and analyzed,with focus on the inherent compositions and work function.Then the MoO_(x) films are applied into SHJ solar cells.When the MoO_(x) works as a buffer layer between ITO/p-a-Si:H interface in the reference SHJ solar cell,a conversion efficiency of 19.1%can be obtained.When the MoOx is used as a hole transport layer(HTL),the device indicates a desirable conversion efficiency of 17.5%.To the best of our knowledge,this current efficiency is the highest one for the MoO_(x) film as HTL by RF sputtering.
文摘The laser equipment is one of the key equipment in the production line of the solar energy. In this article, the author de-scribes the application of the laser equipment in the production line of the amorphous silicon film solar cells, and points out that the stable and exactitude is the key direction of the future development of the laser scribing equipment.
基金Project supported by the Key-Area Research and Development Program of Guangdong Province,China (Grant No.2021B0101260001)Guangdong Basic and Applied Basic Research Foundation (Grant No.2019A1515110411)the National Natural Science Foundation of China (Grant No.61904201)。
文摘Silicon passivated emitter and rear contact(PERC) solar cells with V-groove texture were fabricated using maskless alkaline solution etching with in-house developed additive. Compared with the traditional pyramid texture, the V-groove texture possesses superior effective minority carrier lifetime, enhanced p–n junction quality and better applied filling factor(FF). In addition, a V-groove texture can greatly reduce the shading area and edge damage of front Ag electrodes when the V-groove direction is parallel to the gridline electrodes. Due to these factors, the V-groove solar cells have a higher efficiency(21.78%) than pyramid solar cells(21.62%). Interestingly, external quantum efficiency(EQE) and reflectance of the V-groove solar cells exhibit a slight decrease when the incident light angle(θ) is increased from 0° to 75°, which confirms the excellent quasi omnidirectionality of the V-groove solar cells. The proposed V-groove solar cell design shows a 2.84% relative enhancement of energy output over traditional pyramid solar cells.
文摘This article presents a three-dimensional analysis of the impact of the angle of incidence of the magnetic field intensity on the electrical performance (series resistance, shunt resistance) of a bifacial polycrystalline silicon solar cell. The cell is illuminated simultaneously from both sides. The continuity equation for the excess minority carriers is solved at the emitter and at the depth of the base respectively. The analytical expressions for photocurrent density, photovoltage, series resistance and shunt resistance were deduced. Using these expressions, the values of the series and shunt resistances were extracted for different values of the angle of incidence of the magnetic field intensity. The study shows that as the angle of incidence increases, the slopes of the minority carrier density for the two modes of operation of the solar cell decrease. This is explained by a drop in the accumulation of carriers in the area close to the junction due to the fact that the Lorentz force is unable to drive the carriers towards the lateral surfaces due to the weak action of the magnetic field, which tends to cancel out as the incidence angle increases, and consequently a drop in the open circuit photovoltage. This, in turn, reduces the Lorentz force. These results predict that the p-n junction of the solar cell will not heat up. The study also showed a decrease in series resistance as the incidence angle of the magnetic field intensity increased from 0 rad to π/2 rad and an increase in shunt resistance as the incidence angle increased. His behaviour of the electrical parameters when the angle of incidence of the field from 0 rad to π/2 rad shows that the decreasing magnetic field vector tends to be collinear with the electron trajectory. This allows them to cross the junction and participate in the external current. The best orientation for the Lorentz force is zero, in which case the carriers can move easily towards the junction.
文摘By solving the magneto-transport equation for excess minority charge carriers in the base of the series vertical-junction silicon cell, the phenomenological parameters of the cell can be determined from the boundary conditions. Photocurrent density and photovoltage are determined for each value of applied magnetic field and corresponding optimum thickness, to establish the current-voltage characteristic (Jph(Sf, Sb, z, B, Hop)-Vph(Sf, Sb, z, B, Hop) of the silicon cell under polychromatic illumination. This study will make it possible to reduce the material used (by reducing the optimum thickness), which will help to lower prices. It will also enable us to reduce betting effects (lower series resistance), thereby boosting solar cell efficiency.