The possibility of a life prediction model for nickel base single crystal blades has been studied. The fatigue creep (FC) and thermal fatigue creep(TMFC) as well as creep experiments have been carried out with differe...The possibility of a life prediction model for nickel base single crystal blades has been studied. The fatigue creep (FC) and thermal fatigue creep(TMFC) as well as creep experiments have been carried out with different hold time of DD3. The hold time and the frequency as well as the temperature range are the main factors influencing the life. An emphasis has been put on the micro mechanism of the rupture of creep, FC and TMFC. Two main factors are the voiding and degeneration of the material for the cre...展开更多
基金National Natural Science F oundation of China (5 0 0 0 5 0 16) Aviation F oundation (0 0 B5 3 0 10 ) as well as theYangtze River Foundation
文摘The possibility of a life prediction model for nickel base single crystal blades has been studied. The fatigue creep (FC) and thermal fatigue creep(TMFC) as well as creep experiments have been carried out with different hold time of DD3. The hold time and the frequency as well as the temperature range are the main factors influencing the life. An emphasis has been put on the micro mechanism of the rupture of creep, FC and TMFC. Two main factors are the voiding and degeneration of the material for the cre...