The service performance of the turbine blade root of an aero-engine depends on the microstructures in its superficial layer.This work investigated the surface deformation structures of turbine blade root of single cry...The service performance of the turbine blade root of an aero-engine depends on the microstructures in its superficial layer.This work investigated the surface deformation structures of turbine blade root of single crystal nickel-based superalloy produced under different creep feed grinding conditions.Gradient microstructures in the superficial layer were clarified and composed of a severely deformed layer(DFL)with nano-sized grains(48–67 nm)at the topmost surface,a DFL with submicron-sized grains(66–158 nm)and micron-sized laminated structures at the subsurface,and a dislocation accumulated layer extending to the bulk material.The formation of such gradient microstructures was found to be related to the graded variations in the plastic strain and strain rate induced in the creep feed grinding process,which were as high as 6.67 and 8.17×10^(7)s^(−1),respectively.In the current study,the evolution of surface gradient microstructures was essentially a transition process from a coarse single crystal to nano-sized grains and,simultaneously,from one orientation of a single crystal to random orientations of polycrystals,during which the dislocation slips dominated the creep feed grinding induced microstructure deformation of single crystal nickel-based superalloy.展开更多
The oxidation behavior of a novel Ni-based single-crystal 4774DD1 superalloy for industrial gas turbine applications was investigated by the isothermal oxidation at 980℃ and discontinuous oxidation weight gain method...The oxidation behavior of a novel Ni-based single-crystal 4774DD1 superalloy for industrial gas turbine applications was investigated by the isothermal oxidation at 980℃ and discontinuous oxidation weight gain methods.The phase constitution and morphology of surface oxides and the characteristics of the crosssection oxide film were analyzed by XRD,SEM and EDS.Results show that the oxidation kinetics of the 4774DD1 superalloy follows the cubic law,indicating its weak oxidation resistance at this temperature.As the oxidation time increases,the composition of the oxide film evolves as following:One layer consisting of a bottom Al_(2)O_(3)sublayer and an upper(Al_(2)O_(3)+NiO)mixture sublayer after oxidized for 25 h.Then,two layers composed of an outermost small NiO discontinuous grain layer and an internal layer for 75 h.This internal layer is consisted of the bottom Al_(2)O_(3)sublayer,an intermediate narrow CrTaO_(4)sublayer,and an upper(Al_(2)O_(3)+NiO)mixture sublayer.Also two layers comprising an outermost relative continuous NiO layer with large grain size and an internal layer as the oxidation time increases to 125 h.This internal layer is composed of the upper(Al_(2)O_(3)+NiO)mixture sublayer,an intermediate continuous(CrTaO_(4)+NiWO_(4))mixture sublayer,and a bottom Al_(2)O_(3)sublayer.Finally,three layers consisting of an outermost(NiAl2O_(4)+NiCr2O_(4))mixture layer,an intermediate(CrTaO_(4)+NiWO_(4))mixture layer,and a bottom Al_(2)O_(3)layer for 200 h.展开更多
The influence of temperatures on the stacking fault energies and deformation mechanism of a Re- containing single crystal nickel-based superalloy during creep at elevated temperatures was investigated by means of calc...The influence of temperatures on the stacking fault energies and deformation mechanism of a Re- containing single crystal nickel-based superalloy during creep at elevated temperatures was investigated by means of calculating the stacking fault energy of alloy, measuring creep properties and performing contrast analysis of dislocation configuration. The results show that the alloy at 760 ℃ possesses lower stacking fault energy, and the stacking fault of alloy increases with increasing temperature. The defor- mation mechanism of alloy during creep at 760 ℃ is 7' phase sheared by 〈110〉 super-dislocations, which may be decomposed to form the configuration of Shockley partials plus super-lattice intrinsic stacking fault, while the deformation mechanism of alloy during creep at 1070 ℃ is the screw or edge super- dislocations shearing into the rafted 7' phase. But during creep at 7(50 and 980 ℃, some super- dislocations shearing into 7' phase may cross-slip from the {111} to {100} planes to form the K-W locks with non-plane core structure, which may restrain the dislocations slipping to enhance the creep resis- tance of alloy at high temperature. The interaction between the Re and other elements may decrease the diffusion rate of atoms to improve the microstructure stability, which is thought to be the main reason why the K-W locks are to be kept in the Re-containing superalloy during creep at 980 ℃.展开更多
A series of experiments of investigating the recrystallization of single crystal DD3 superalloy were carried out. The threshold temperature for recrystallization and the effect of annealing temperature on recrystalliz...A series of experiments of investigating the recrystallization of single crystal DD3 superalloy were carried out. The threshold temperature for recrystallization and the effect of annealing temperature on recrystallization were studied. The results show that the threshold temperature for recrystallization of the shot-peened DD3 samples is between 1 000 ℃ and 1 050 ℃ under the condition of annealing for 2 h, and the recrystallization depth increases with the rise of the annealing temperature. Below 1 150 ℃, the recrystallization depth increases slowly with the temperature climbing, while above 1 150 ℃, the recrystallization depth increases quickly with the rise of the temperature. The solution of the γ' phase is a critical factor of the recrystallization behavior of DD3 superalloy. In addition, the kinetics and microstructural evolution of recrystallization at 1 200 ℃ were also studied. It is found that the recrystallization progresses rapidly at 1 200 ℃ through the growth of fully developed recrystallized grains, and the recrystallization process on the shot-peened surface is similar to that of wrought materials, including nucleation of recrystallization, growth of new grains into the matrix, and growth of new grains by swallowing up each other.展开更多
The low-cycle fatigue (LCF) behavior of a nickel-based single crystal superalloy with [001] orientation was studied at an intermediate temperature of T0℃ and a higher temperature of To + 250℃ under a constant low...The low-cycle fatigue (LCF) behavior of a nickel-based single crystal superalloy with [001] orientation was studied at an intermediate temperature of T0℃ and a higher temperature of To + 250℃ under a constant low strain rate of 10^-3 s^-1 in ambient atmosphere. The superalloy exhibited cyclic tension-compression asymmetry which is dependent on the temperature and applied strain amplitude. Analysis on the fracture surfaces showed that the surface and subsurface casting micropores were the major crack initiation sites. Interior Ta-rich carbides were frequently observed in all specimens. Two distinct types of fracture were suggested by fractogaphy. One type was characterized by Mode-I cracking with a microscopically rough surface at To + 250℃. Whereas the other type at lower temperature T0℃ favored either one or several of the octahedral {111} planes, in contrast to the normal Mode-I growth mode typically observed at low loading frequencies (several Hz). The failure mechanisms for two cracking modes are shearing of γ' precipitates together with the matrix at T0℃ and cracking confined in the matrix and the γ/γ'interface at To - 250℃.展开更多
The crystal growth of a nickel-based single crystal superalloy DD3 was researched via controlled directional solidification under the action of a DC electric field. The cellular or dendrite spacing of the single cryst...The crystal growth of a nickel-based single crystal superalloy DD3 was researched via controlled directional solidification under the action of a DC electric field. The cellular or dendrite spacing of the single crystal superalloy is refined and microsegregation of alloying elements Al, Ti, Mo and W, is reduced by the electric field. The electric field decreases the interface stability and reduces the critical growth rate of the ceUular-dendritic translation because of Thomson effect and Joule heating. The precipitation of the γ' phase is more uniform and the size of the γ' phase is smaller with the electric field than that without the electric field.展开更多
Low cycle fatigue tests were conducted on the single crystal nickel-based superalloy, DD6, with different crystallographic orientations (i.e., [001], [011], and [111]) and strain dwell types (i.e, tensile, compress...Low cycle fatigue tests were conducted on the single crystal nickel-based superalloy, DD6, with different crystallographic orientations (i.e., [001], [011], and [111]) and strain dwell types (i.e, tensile, compressive, and balanced types) at a certain high temperature. Given the material anisotropy and mean stress, both orientation factor and stress range were introduced to the Smith, Watson, and Topper (SWT) stress model to predict the fatigue life. Experimental results indicated that the fatigue properties of DD6 depend on both crystallographic orientation and loading types. The fatigue life of the tensile, compressive, and balanced strain dwell tests are shorter than those of continuous cycling tests without strain dwell because of the important creep effect. The predicted results of the proposed modified SWT stress method agree well with the experimental data.展开更多
The evolution of micro-pores in a single crystal nickel-based superalloy during creep at 980 ℃/220 MPa was investigated by X-ray computed tomography. Time-dependent ex-situ 3D information including the number, volume...The evolution of micro-pores in a single crystal nickel-based superalloy during creep at 980 ℃/220 MPa was investigated by X-ray computed tomography. Time-dependent ex-situ 3D information including the number, volume fraction, distribution and morphology of micro-pores was analyzed. The results reveal that the signifi cant formation and growth of micro-pores occur at the end of secondary/beginning of tertiary creep stage. The irregular large pores as well as high density pores located at strain concentration region are the major detrimental factors facilitating the creep damage. Creep failure is resulted from the connection of surface cracks induced by oxidation, and the internal cracks generated from growth and merging of micro-pores.展开更多
The recrystallization behaviors of a nickel-based single crystal superalloy during heat treatment at 1,200℃ for 4 h with various cooling rates were studied.Results show that the thickness of recrystallization layer d...The recrystallization behaviors of a nickel-based single crystal superalloy during heat treatment at 1,200℃ for 4 h with various cooling rates were studied.Results show that the thickness of recrystallization layer decreases with the increase of cooling rate.In addition,the microstructures ofγ′phase in the recrystallization region are different in various cooling rates.In the high cooling rates(70,100℃·min^(-1)),small size and high volume fraction ofγ′phases are formed in the recrystallization region.It is also found that irregular fine secondaryγ′phases are precipitated between matrix channels with an average size of 150 nm in the original matric(100℃·min^(-1)).The sizes of the secondaryγ′phase decrease with the increase of cooling rate.In contrast,large size and small volume fraction ofγ′phases are formed in the recrystallization region,and a grain boundary layer is formed under a low cooling rate(10℃·min^(-1)).The evolution mechanism of recrystallization at various cooling rates during heat treatment is analyzed.展开更多
Directionally solidified single crystal superalloy test bars were prepared by the spiral grain selection method.The microstructural evolution and orientation characteristics of the starter block and spiral part were s...Directionally solidified single crystal superalloy test bars were prepared by the spiral grain selection method.The microstructural evolution and orientation characteristics of the starter block and spiral part were studied,and the influence of the competitive growth of crystals on the microstructural characteristics was analyzed.The results show that the divergent grain groups,with small size and randomly oriented grains,appear at the bottom of the start block due to the chilling effect,which is an important area for competitive growth.As the height of the starter block increases,the primary dendrite spacing increases,and the grain density decreases;furthermore,the proportion of grains with an orientation deflection angle less than 10°gradually increases.The<001>texture gradually becomes stronger as the height of the starter block increases,which indicates that the competitive growth of crystals gradually weakens.At the initial stage of the crystal selection in the spiral part,the obstacle of adjacent grains and spiral passage is the main working mechanism.The grains located at the inner side of the front edge of the spiral passage have the growth advantage.The single crystal screening process is achieved at about two-thirds of the spiral height,and the single crystal with the orientation deviation angle of 6.7°from the casting axis is prepared.展开更多
The recrystallization behavior of a single crystal nickel-base superalloy was investigated by shot peening and subsequent annealing. Two kinds of recrystallization microstructures, which are intensively dependent on t...The recrystallization behavior of a single crystal nickel-base superalloy was investigated by shot peening and subsequent annealing. Two kinds of recrystallization microstructures, which are intensively dependent on the annealing temperature, are shown in the nickel-base superalloy after shot peening and subsequent annealing. Surface recrystallized grains are obtained when the superalloy is annealed at solution treatment temperature. The nucleation of recrystallization originates from the dendritic core, where rapid dissolution of γ' particles occurs. Cellular recrystallization is observed after annealing at lower temperatures. Cellular structures induced by high diffusivity of the moving boundary and more γ' particles dissolution led by residual stress are developed from the surface region. Recrystallized kinetics of the shot-peened alloy annealed at 1050°C accords with the Johnson-Mehl-Avrami-Kolmogorov equation. The low Avrami exponent is caused by the inhomogeneous distribution of stored energy, the decreasing of stored energy during recovery, and the strong resistance of boundary migration by γ' particles.展开更多
Fully reversed low cyclic fatigue (LCF) tests were conducted on [0 0 1], [0 1 2], [(1) over bar 1 2], [0 1 1] and [(1) over bar 1 4] oriented single crystals of nickel-bared superalloy DD3 with different cyclic strain...Fully reversed low cyclic fatigue (LCF) tests were conducted on [0 0 1], [0 1 2], [(1) over bar 1 2], [0 1 1] and [(1) over bar 1 4] oriented single crystals of nickel-bared superalloy DD3 with different cyclic strain rates at 950 degrees C. The cyclic strain rates were chosen as 1.0 x 10(-2), 1.33 x 10(-3) and 0.33 x 10(-3) s(-1). The octahedral slip systems were confirmed to be activated on all the specimens. The experimental result shows that the fatigue behavior depends an the crystallographic orientation and cyclic strain rate. Except [0 0 1] orientation specimens, it is found from the scanning electron microscopy(SEM) examination that there are typical fatigue striations on the fracture surfaces. These fatigue striations are made up of cracks. The width of the fatigue striations depends on the crystallographic orientation and varies with the total strain range. A simple linear relationship exists between the width and total shear strain range modified by an orientation and strain rate parameter. The nonconformity to the Schmid law of tensile/compressive flaw stress and plastic behavior existed at 95 degrees C, and an orientation and strain rate modified Lall-Chin-Pope ( LCP) model was derived for the nonconformity. The influence of crysrallographic orientation and cyclic strain rate on the LCF behavior can be predicted satisfactorily by the model. In terms of an orientation and strain rate modified total strain range, a model for fatigue life was proposed and used successfully to correlate the fatigue lives studied.展开更多
By means of pre-compressive creep treatment, the cubic γ′ phase in a nickel base single crystal superalloy is transformed into the P-type rafted structure. And the influence of the pre-compressive creep on the inter...By means of pre-compressive creep treatment, the cubic γ′ phase in a nickel base single crystal superalloy is transformed into the P-type rafted structure. And the influence of the pre-compressive creep on the internal friction stress and creep lifetimes of the superalloy are investigated by means of the measurement of the creep curves and microstructure observation. Results show that, compared to the P-type structure alloy, the full heat treated state alloy displays a bigger internal friction stress value of dislocation motion during steady state creep and a longer creep lifetimes. The creep activation energies of the full heat treated and P-type structures alloys are measured to be 462 kJ/mol and 412 kJ/mol, respectively. Thereinto, the P-type rafted γ′ phase in the alloy is transformed into the N-type structure during tensile creep. And the N-type γ′ phase transformed from the P-type structure displays a shorter size in length, this is a main reason of the P-type structure alloy possessing a shorter creep lifetimes due to creep dislocation moving easily over the rafted γ′ phase.展开更多
Numerical calculations of creep damage development and life behavior of circular notched specimens of nickel-base single crystal had been performed. The creep stress distributions depend on the specimen geometry. For ...Numerical calculations of creep damage development and life behavior of circular notched specimens of nickel-base single crystal had been performed. The creep stress distributions depend on the specimen geometry. For a small notch radius, von Mises stress has an especial distribution. The damage distribution is greatly influenced by the notch depth, notch radius as well as notch type. The creep crack initiation place is different for each notched specimen. The characteristics of notch strengthening and notch weakening depend on the notch radius and notch type. For the same notch type, the creep rupture lives decrease with the decreasing of notch radius. A creep life model has been presented for the multiaxial stress states based on the crystallographic slip system theory.展开更多
An investigation has been made into strengthening mechanism in a single crystal nickel-base superalloy DD8 by transmission electron microscopy. The results show that the stress rupture strength of the alloy increases ...An investigation has been made into strengthening mechanism in a single crystal nickel-base superalloy DD8 by transmission electron microscopy. The results show that the stress rupture strength of the alloy increases with decreasing misfit, and the antiphase boundaries (APBs) formed in the ordered γ' phase, rather than the misfits, play a dominate role in strengthening of the single crystal Ni-base superalloy DD8.There are three kinds of mechanisms for forming the APBs which were observed in the present materials. One is mis-arrangement of the local ordered atoms in the γ' precipitates due to the local strain; the second arises from the 1/2<110> dislocations cutting into the γ', and the third is the formation of the APBs induced by the 1/2<110> matrix dislocation network. The contribution of the antiphase boundary energy to the strength of the alloy can be expressed by:where τ is the resistance to deformation provided by the APB energy; S is the long-range order degree in γ'; Tc is the transition temperature from order to disorder; f is the volume fraction of γ'; rs is the radius of γ'; b is the Burgers vector; a is the lattice constant; G is the shear modulus, and k is the proportional constant.展开更多
The creep and rupture behavior of a nickel-base single crystal superalloy with [001] orientation was investigated at temperature of 10001040℃ and stress in the range of 150320MPa. The creep features and micro...The creep and rupture behavior of a nickel-base single crystal superalloy with [001] orientation was investigated at temperature of 10001040℃ and stress in the range of 150320MPa. The creep features and microstructure were studied by means of the measurement of creep curves and TEM observation. The results show that all creep curves exhibit a short primary and a dominant accelerated creep stage. From the creep parameters and TEM observations, it is suggested that the primary deformation mechanism has a change from precipitatation shearing by pairs of dislocation in the high applied stress region to dislocations climb around the γ′ particles in the low applied stress region. Furthermore, the detailed failure process and fracture surfaces were analyzed by SEM observation.展开更多
High-cycle rotating bending fatigue behavior of SRR99 nickel-base single crystal alloy at 700 and 900℃ was investigated. The fatigue strengths for 107 cycles are 350 and 335MPa at 700 and 900℃, respectively. T...High-cycle rotating bending fatigue behavior of SRR99 nickel-base single crystal alloy at 700 and 900℃ was investigated. The fatigue strengths for 107 cycles are 350 and 335MPa at 700 and 900℃, respectively. The total fatigue life becomes shorter when the temperature increases regardless of the loading stress and frequency. With the number of cycles decreasing, the difference in fatigue strength at the two temperatures becomes smaller. Typical fatigue rupture process including crack initiation site, crack propagation region and final rupture region exhibits at 700℃. The fracture surface is basically characterized by cleavage rupture at 900℃.展开更多
Microstructure evolution of a single crystal nickel-base superalloy during heat treatment and tensile creep at 1010°C and 248 MPa for 30h was observed and analyzed. Internal stresses because of lattice mismatch b...Microstructure evolution of a single crystal nickel-base superalloy during heat treatment and tensile creep at 1010°C and 248 MPa for 30h was observed and analyzed. Internal stresses because of lattice mismatch between and / phase provided the driving force for / shape evolution during heat treatment. More than 65 vol. % distorted cubic phase keeping coherency with the y matrix precipitated after solution at 1295°C for 32h. The shape of phase was perfectly cubic with increasing precipitate size during the two-step aging treatment. Due to the applied stress and internal stress field the continuous y1/ lamellar structure perpendicular to the applied stress was formed after 30h tensile creep.展开更多
基金This work was financially supported by the National Nat-ural Science Foundation of China(Nos.51921003,51775275 and 51905363)the Natural Science Foundation of Jiangsu Province(No.BK20190940)+1 种基金the National Major Science and Technology Projects of China(No.2017-VII-0002-0095)the Six Talents Summit Project in Jiangsu Province(No.JXQC-002).
文摘The service performance of the turbine blade root of an aero-engine depends on the microstructures in its superficial layer.This work investigated the surface deformation structures of turbine blade root of single crystal nickel-based superalloy produced under different creep feed grinding conditions.Gradient microstructures in the superficial layer were clarified and composed of a severely deformed layer(DFL)with nano-sized grains(48–67 nm)at the topmost surface,a DFL with submicron-sized grains(66–158 nm)and micron-sized laminated structures at the subsurface,and a dislocation accumulated layer extending to the bulk material.The formation of such gradient microstructures was found to be related to the graded variations in the plastic strain and strain rate induced in the creep feed grinding process,which were as high as 6.67 and 8.17×10^(7)s^(−1),respectively.In the current study,the evolution of surface gradient microstructures was essentially a transition process from a coarse single crystal to nano-sized grains and,simultaneously,from one orientation of a single crystal to random orientations of polycrystals,during which the dislocation slips dominated the creep feed grinding induced microstructure deformation of single crystal nickel-based superalloy.
基金supported by the fund of State Key Laboratory of Long-life High Temperature Materials(Grant No.DTCC28EE200787)the Natural Science Basic Research Plan in Shaanxi Province of China(Grant No.2022JQ-553)+3 种基金the China Postdoctoral Science Foundation(Grant No.2021M692555)the Excellent Youth Foundation of Shaanxi Province of China(Grant No.2021JC-08)the Beilin district of Xi’an Science and Technology Project(Grant No.GX2123)the support from the Youth Innovation Team of Shaanxi Universities。
文摘The oxidation behavior of a novel Ni-based single-crystal 4774DD1 superalloy for industrial gas turbine applications was investigated by the isothermal oxidation at 980℃ and discontinuous oxidation weight gain methods.The phase constitution and morphology of surface oxides and the characteristics of the crosssection oxide film were analyzed by XRD,SEM and EDS.Results show that the oxidation kinetics of the 4774DD1 superalloy follows the cubic law,indicating its weak oxidation resistance at this temperature.As the oxidation time increases,the composition of the oxide film evolves as following:One layer consisting of a bottom Al_(2)O_(3)sublayer and an upper(Al_(2)O_(3)+NiO)mixture sublayer after oxidized for 25 h.Then,two layers composed of an outermost small NiO discontinuous grain layer and an internal layer for 75 h.This internal layer is consisted of the bottom Al_(2)O_(3)sublayer,an intermediate narrow CrTaO_(4)sublayer,and an upper(Al_(2)O_(3)+NiO)mixture sublayer.Also two layers comprising an outermost relative continuous NiO layer with large grain size and an internal layer as the oxidation time increases to 125 h.This internal layer is composed of the upper(Al_(2)O_(3)+NiO)mixture sublayer,an intermediate continuous(CrTaO_(4)+NiWO_(4))mixture sublayer,and a bottom Al_(2)O_(3)sublayer.Finally,three layers consisting of an outermost(NiAl2O_(4)+NiCr2O_(4))mixture layer,an intermediate(CrTaO_(4)+NiWO_(4))mixture layer,and a bottom Al_(2)O_(3)layer for 200 h.
基金supported by the National Natural Science Foundation of China (Grant No. 51271125)
文摘The influence of temperatures on the stacking fault energies and deformation mechanism of a Re- containing single crystal nickel-based superalloy during creep at elevated temperatures was investigated by means of calculating the stacking fault energy of alloy, measuring creep properties and performing contrast analysis of dislocation configuration. The results show that the alloy at 760 ℃ possesses lower stacking fault energy, and the stacking fault of alloy increases with increasing temperature. The defor- mation mechanism of alloy during creep at 760 ℃ is 7' phase sheared by 〈110〉 super-dislocations, which may be decomposed to form the configuration of Shockley partials plus super-lattice intrinsic stacking fault, while the deformation mechanism of alloy during creep at 1070 ℃ is the screw or edge super- dislocations shearing into the rafted 7' phase. But during creep at 7(50 and 980 ℃, some super- dislocations shearing into 7' phase may cross-slip from the {111} to {100} planes to form the K-W locks with non-plane core structure, which may restrain the dislocations slipping to enhance the creep resis- tance of alloy at high temperature. The interaction between the Re and other elements may decrease the diffusion rate of atoms to improve the microstructure stability, which is thought to be the main reason why the K-W locks are to be kept in the Re-containing superalloy during creep at 980 ℃.
基金Item Sponsored by Open Foundation of Nondestructive Test Key Laboratory of Chinese Ministry of Education(ZD200729011)
文摘A series of experiments of investigating the recrystallization of single crystal DD3 superalloy were carried out. The threshold temperature for recrystallization and the effect of annealing temperature on recrystallization were studied. The results show that the threshold temperature for recrystallization of the shot-peened DD3 samples is between 1 000 ℃ and 1 050 ℃ under the condition of annealing for 2 h, and the recrystallization depth increases with the rise of the annealing temperature. Below 1 150 ℃, the recrystallization depth increases slowly with the temperature climbing, while above 1 150 ℃, the recrystallization depth increases quickly with the rise of the temperature. The solution of the γ' phase is a critical factor of the recrystallization behavior of DD3 superalloy. In addition, the kinetics and microstructural evolution of recrystallization at 1 200 ℃ were also studied. It is found that the recrystallization progresses rapidly at 1 200 ℃ through the growth of fully developed recrystallized grains, and the recrystallization process on the shot-peened surface is similar to that of wrought materials, including nucleation of recrystallization, growth of new grains into the matrix, and growth of new grains by swallowing up each other.
基金supported by the National Natural Science Foundation of China(No.50371042).
文摘The low-cycle fatigue (LCF) behavior of a nickel-based single crystal superalloy with [001] orientation was studied at an intermediate temperature of T0℃ and a higher temperature of To + 250℃ under a constant low strain rate of 10^-3 s^-1 in ambient atmosphere. The superalloy exhibited cyclic tension-compression asymmetry which is dependent on the temperature and applied strain amplitude. Analysis on the fracture surfaces showed that the surface and subsurface casting micropores were the major crack initiation sites. Interior Ta-rich carbides were frequently observed in all specimens. Two distinct types of fracture were suggested by fractogaphy. One type was characterized by Mode-I cracking with a microscopically rough surface at To + 250℃. Whereas the other type at lower temperature T0℃ favored either one or several of the octahedral {111} planes, in contrast to the normal Mode-I growth mode typically observed at low loading frequencies (several Hz). The failure mechanisms for two cracking modes are shearing of γ' precipitates together with the matrix at T0℃ and cracking confined in the matrix and the γ/γ'interface at To - 250℃.
基金supported by the National Natural Science Foundation of China(No.50374062)the Science and Technology Foundation of Liaoning(No.20032015).
文摘The crystal growth of a nickel-based single crystal superalloy DD3 was researched via controlled directional solidification under the action of a DC electric field. The cellular or dendrite spacing of the single crystal superalloy is refined and microsegregation of alloying elements Al, Ti, Mo and W, is reduced by the electric field. The electric field decreases the interface stability and reduces the critical growth rate of the ceUular-dendritic translation because of Thomson effect and Joule heating. The precipitation of the γ' phase is more uniform and the size of the γ' phase is smaller with the electric field than that without the electric field.
基金The financial support for this work from the National Natural Science Foundation of China (Grant No. 51341001) is appreciated.
文摘Low cycle fatigue tests were conducted on the single crystal nickel-based superalloy, DD6, with different crystallographic orientations (i.e., [001], [011], and [111]) and strain dwell types (i.e, tensile, compressive, and balanced types) at a certain high temperature. Given the material anisotropy and mean stress, both orientation factor and stress range were introduced to the Smith, Watson, and Topper (SWT) stress model to predict the fatigue life. Experimental results indicated that the fatigue properties of DD6 depend on both crystallographic orientation and loading types. The fatigue life of the tensile, compressive, and balanced strain dwell tests are shorter than those of continuous cycling tests without strain dwell because of the important creep effect. The predicted results of the proposed modified SWT stress method agree well with the experimental data.
基金supported by the National Natural Science Foundation of China(Grant Nos.51631008,91860201,51771204,51911530154 and U1732131)the National Science and Technology Major Project(2017-VII-0008-0101,2017-VI0003-0073 and J2019-VI-0010)the Key Deployment Projects of the Chinese Academy of Sciences(ZDRW-CN-2019-01)。
文摘The evolution of micro-pores in a single crystal nickel-based superalloy during creep at 980 ℃/220 MPa was investigated by X-ray computed tomography. Time-dependent ex-situ 3D information including the number, volume fraction, distribution and morphology of micro-pores was analyzed. The results reveal that the signifi cant formation and growth of micro-pores occur at the end of secondary/beginning of tertiary creep stage. The irregular large pores as well as high density pores located at strain concentration region are the major detrimental factors facilitating the creep damage. Creep failure is resulted from the connection of surface cracks induced by oxidation, and the internal cracks generated from growth and merging of micro-pores.
基金financially supported by the National Natural Science Foundation of China(No.92060104)the National Science and Technology Major Project(No.2017-VII-00080102)the Shanghai Municipal Science and Technology Committee Grant(No.20511107700)。
文摘The recrystallization behaviors of a nickel-based single crystal superalloy during heat treatment at 1,200℃ for 4 h with various cooling rates were studied.Results show that the thickness of recrystallization layer decreases with the increase of cooling rate.In addition,the microstructures ofγ′phase in the recrystallization region are different in various cooling rates.In the high cooling rates(70,100℃·min^(-1)),small size and high volume fraction ofγ′phases are formed in the recrystallization region.It is also found that irregular fine secondaryγ′phases are precipitated between matrix channels with an average size of 150 nm in the original matric(100℃·min^(-1)).The sizes of the secondaryγ′phase decrease with the increase of cooling rate.In contrast,large size and small volume fraction ofγ′phases are formed in the recrystallization region,and a grain boundary layer is formed under a low cooling rate(10℃·min^(-1)).The evolution mechanism of recrystallization at various cooling rates during heat treatment is analyzed.
基金financially supported by the National Natural Science Foundation of China (52071065)the National Key Research and Development Program of China (2016YFB0301201)the Fundamental Research Funds for the Central Universities (N2007007)
文摘Directionally solidified single crystal superalloy test bars were prepared by the spiral grain selection method.The microstructural evolution and orientation characteristics of the starter block and spiral part were studied,and the influence of the competitive growth of crystals on the microstructural characteristics was analyzed.The results show that the divergent grain groups,with small size and randomly oriented grains,appear at the bottom of the start block due to the chilling effect,which is an important area for competitive growth.As the height of the starter block increases,the primary dendrite spacing increases,and the grain density decreases;furthermore,the proportion of grains with an orientation deflection angle less than 10°gradually increases.The<001>texture gradually becomes stronger as the height of the starter block increases,which indicates that the competitive growth of crystals gradually weakens.At the initial stage of the crystal selection in the spiral part,the obstacle of adjacent grains and spiral passage is the main working mechanism.The grains located at the inner side of the front edge of the spiral passage have the growth advantage.The single crystal screening process is achieved at about two-thirds of the spiral height,and the single crystal with the orientation deviation angle of 6.7°from the casting axis is prepared.
基金supported by the Major State Basic Research and Development Program of China (No.2010CB631206)the National Natural Science Foundation of China (No.50931004)the Foundation of State Key Lab for Advanced Metals and Materials (No.2008zd-07)
文摘The recrystallization behavior of a single crystal nickel-base superalloy was investigated by shot peening and subsequent annealing. Two kinds of recrystallization microstructures, which are intensively dependent on the annealing temperature, are shown in the nickel-base superalloy after shot peening and subsequent annealing. Surface recrystallized grains are obtained when the superalloy is annealed at solution treatment temperature. The nucleation of recrystallization originates from the dendritic core, where rapid dissolution of γ' particles occurs. Cellular recrystallization is observed after annealing at lower temperatures. Cellular structures induced by high diffusivity of the moving boundary and more γ' particles dissolution led by residual stress are developed from the surface region. Recrystallized kinetics of the shot-peened alloy annealed at 1050°C accords with the Johnson-Mehl-Avrami-Kolmogorov equation. The low Avrami exponent is caused by the inhomogeneous distribution of stored energy, the decreasing of stored energy during recovery, and the strong resistance of boundary migration by γ' particles.
文摘Fully reversed low cyclic fatigue (LCF) tests were conducted on [0 0 1], [0 1 2], [(1) over bar 1 2], [0 1 1] and [(1) over bar 1 4] oriented single crystals of nickel-bared superalloy DD3 with different cyclic strain rates at 950 degrees C. The cyclic strain rates were chosen as 1.0 x 10(-2), 1.33 x 10(-3) and 0.33 x 10(-3) s(-1). The octahedral slip systems were confirmed to be activated on all the specimens. The experimental result shows that the fatigue behavior depends an the crystallographic orientation and cyclic strain rate. Except [0 0 1] orientation specimens, it is found from the scanning electron microscopy(SEM) examination that there are typical fatigue striations on the fracture surfaces. These fatigue striations are made up of cracks. The width of the fatigue striations depends on the crystallographic orientation and varies with the total strain range. A simple linear relationship exists between the width and total shear strain range modified by an orientation and strain rate parameter. The nonconformity to the Schmid law of tensile/compressive flaw stress and plastic behavior existed at 95 degrees C, and an orientation and strain rate modified Lall-Chin-Pope ( LCP) model was derived for the nonconformity. The influence of crysrallographic orientation and cyclic strain rate on the LCF behavior can be predicted satisfactorily by the model. In terms of an orientation and strain rate modified total strain range, a model for fatigue life was proposed and used successfully to correlate the fatigue lives studied.
基金Supported by the National Natural Science Foundation of China (No 50571070)
文摘By means of pre-compressive creep treatment, the cubic γ′ phase in a nickel base single crystal superalloy is transformed into the P-type rafted structure. And the influence of the pre-compressive creep on the internal friction stress and creep lifetimes of the superalloy are investigated by means of the measurement of the creep curves and microstructure observation. Results show that, compared to the P-type structure alloy, the full heat treated state alloy displays a bigger internal friction stress value of dislocation motion during steady state creep and a longer creep lifetimes. The creep activation energies of the full heat treated and P-type structures alloys are measured to be 462 kJ/mol and 412 kJ/mol, respectively. Thereinto, the P-type rafted γ′ phase in the alloy is transformed into the N-type structure during tensile creep. And the N-type γ′ phase transformed from the P-type structure displays a shorter size in length, this is a main reason of the P-type structure alloy possessing a shorter creep lifetimes due to creep dislocation moving easily over the rafted γ′ phase.
基金supported by the National Natural Science Foundation of China(50005016,50375124)Natural Science Foundation of Shaanxi Province and China Aviation Foundation(02C53011,03B53003)as well as the Yangtze River Foundation
文摘Numerical calculations of creep damage development and life behavior of circular notched specimens of nickel-base single crystal had been performed. The creep stress distributions depend on the specimen geometry. For a small notch radius, von Mises stress has an especial distribution. The damage distribution is greatly influenced by the notch depth, notch radius as well as notch type. The creep crack initiation place is different for each notched specimen. The characteristics of notch strengthening and notch weakening depend on the notch radius and notch type. For the same notch type, the creep rupture lives decrease with the decreasing of notch radius. A creep life model has been presented for the multiaxial stress states based on the crystallographic slip system theory.
文摘An investigation has been made into strengthening mechanism in a single crystal nickel-base superalloy DD8 by transmission electron microscopy. The results show that the stress rupture strength of the alloy increases with decreasing misfit, and the antiphase boundaries (APBs) formed in the ordered γ' phase, rather than the misfits, play a dominate role in strengthening of the single crystal Ni-base superalloy DD8.There are three kinds of mechanisms for forming the APBs which were observed in the present materials. One is mis-arrangement of the local ordered atoms in the γ' precipitates due to the local strain; the second arises from the 1/2<110> dislocations cutting into the γ', and the third is the formation of the APBs induced by the 1/2<110> matrix dislocation network. The contribution of the antiphase boundary energy to the strength of the alloy can be expressed by:where τ is the resistance to deformation provided by the APB energy; S is the long-range order degree in γ'; Tc is the transition temperature from order to disorder; f is the volume fraction of γ'; rs is the radius of γ'; b is the Burgers vector; a is the lattice constant; G is the shear modulus, and k is the proportional constant.
文摘The creep and rupture behavior of a nickel-base single crystal superalloy with [001] orientation was investigated at temperature of 10001040℃ and stress in the range of 150320MPa. The creep features and microstructure were studied by means of the measurement of creep curves and TEM observation. The results show that all creep curves exhibit a short primary and a dominant accelerated creep stage. From the creep parameters and TEM observations, it is suggested that the primary deformation mechanism has a change from precipitatation shearing by pairs of dislocation in the high applied stress region to dislocations climb around the γ′ particles in the low applied stress region. Furthermore, the detailed failure process and fracture surfaces were analyzed by SEM observation.
文摘High-cycle rotating bending fatigue behavior of SRR99 nickel-base single crystal alloy at 700 and 900℃ was investigated. The fatigue strengths for 107 cycles are 350 and 335MPa at 700 and 900℃, respectively. The total fatigue life becomes shorter when the temperature increases regardless of the loading stress and frequency. With the number of cycles decreasing, the difference in fatigue strength at the two temperatures becomes smaller. Typical fatigue rupture process including crack initiation site, crack propagation region and final rupture region exhibits at 700℃. The fracture surface is basically characterized by cleavage rupture at 900℃.
文摘Microstructure evolution of a single crystal nickel-base superalloy during heat treatment and tensile creep at 1010°C and 248 MPa for 30h was observed and analyzed. Internal stresses because of lattice mismatch between and / phase provided the driving force for / shape evolution during heat treatment. More than 65 vol. % distorted cubic phase keeping coherency with the y matrix precipitated after solution at 1295°C for 32h. The shape of phase was perfectly cubic with increasing precipitate size during the two-step aging treatment. Due to the applied stress and internal stress field the continuous y1/ lamellar structure perpendicular to the applied stress was formed after 30h tensile creep.