Physical properties and geometrical morphologies of crushed air-cooled blast furnace slag (SCR) and crushed limestone (LCR) were comparatively investigated. The shape, angularity, surface texture and internal pore...Physical properties and geometrical morphologies of crushed air-cooled blast furnace slag (SCR) and crushed limestone (LCR) were comparatively investigated. The shape, angularity, surface texture and internal pore structure of aggregate particles for different size and gradation were numerically represented by sphericity (ψ) and shape index (SI), angularity number (AN), index of aggregate particle shape and texture (IAPST), porosity and pore size, respectively. The results show that SCR is a porous and rough aggregate. Apparent density, void, water absorption and smashing index of SCR are obviously higher than those of LCR with the same gradation, respectively. However, bulk density of SCR is lower than that of LCR with the same gradation. SI, AN, IAPST and porosity of SCR are obviously higher than those of LCR with the same gradation, respectively. The smaller particle size of SCR, the larger of its AN, IAPST and porosity.展开更多
In order to study the slagging characteristics of boiler combustion liners during pulverized coal stream combustion, the slag samples on the surface of combustion liner were investigated by X-ray diffractometry, scan ...In order to study the slagging characteristics of boiler combustion liners during pulverized coal stream combustion, the slag samples on the surface of combustion liner were investigated by X-ray diffractometry, scan electron microscopy and energy dispersive X-ray analysis, and the transformation characteristics of the compositions and crystal phases were studied. The results show that the size of slag granules decreases as the slagging temperature increases; the crystallinity of coal ash I reduces to about 48.6% when the temperature is increased up to 1 350 ℃, and that of the coal ash II reduces to about 65% when the temperature is increased up to 1 500 ℃; the encroachment of molten coal ash to the combustion liner is strengthened. At the same time, the diffusion and the segregation of the compositions in combustion liners have selectivity, which is in favor of enhancing the content of crystal phases, weakening the conglutination among molten slag compositions and combustion liner, and avoiding yielding big clinkers. But the diffusion of the compositions in combustion liners increases the porosity and decreases the mechanical intensity of combustion liner, and makes the slag encroachment to the liner become more serious.展开更多
基金Funded by the National Basic Research Program of China(No.2009CB623105)the Natural Science Foundation of Education Agency of Anhui Province(No.KJ2012A052)+1 种基金the Anhui Provincial Natural Science Foundation(No.1208085ME82)the Doctor Fund of Anhui University of Architecture(No.20123302)
文摘Physical properties and geometrical morphologies of crushed air-cooled blast furnace slag (SCR) and crushed limestone (LCR) were comparatively investigated. The shape, angularity, surface texture and internal pore structure of aggregate particles for different size and gradation were numerically represented by sphericity (ψ) and shape index (SI), angularity number (AN), index of aggregate particle shape and texture (IAPST), porosity and pore size, respectively. The results show that SCR is a porous and rough aggregate. Apparent density, void, water absorption and smashing index of SCR are obviously higher than those of LCR with the same gradation, respectively. However, bulk density of SCR is lower than that of LCR with the same gradation. SI, AN, IAPST and porosity of SCR are obviously higher than those of LCR with the same gradation, respectively. The smaller particle size of SCR, the larger of its AN, IAPST and porosity.
基金Project(50576005) supported by the National Natural Science Foundation of China
文摘In order to study the slagging characteristics of boiler combustion liners during pulverized coal stream combustion, the slag samples on the surface of combustion liner were investigated by X-ray diffractometry, scan electron microscopy and energy dispersive X-ray analysis, and the transformation characteristics of the compositions and crystal phases were studied. The results show that the size of slag granules decreases as the slagging temperature increases; the crystallinity of coal ash I reduces to about 48.6% when the temperature is increased up to 1 350 ℃, and that of the coal ash II reduces to about 65% when the temperature is increased up to 1 500 ℃; the encroachment of molten coal ash to the combustion liner is strengthened. At the same time, the diffusion and the segregation of the compositions in combustion liners have selectivity, which is in favor of enhancing the content of crystal phases, weakening the conglutination among molten slag compositions and combustion liner, and avoiding yielding big clinkers. But the diffusion of the compositions in combustion liners increases the porosity and decreases the mechanical intensity of combustion liner, and makes the slag encroachment to the liner become more serious.