期刊文献+
共找到186篇文章
< 1 2 10 >
每页显示 20 50 100
Deformation behaviour in advanced heat resistant materials during slow strain rate testing at elevated temperature
1
作者 Mattias Calmunger Guocai Chai +1 位作者 Sten Johansson Johan Moverare 《Theoretical & Applied Mechanics Letters》 CAS 2014年第4期20-25,共6页
In this study, slow strain rate tensile testing at elevated temperature is used to evaluate the influence of temperature and strain rate on deformation behaviour in two different austenitic alloys. One austenitic stai... In this study, slow strain rate tensile testing at elevated temperature is used to evaluate the influence of temperature and strain rate on deformation behaviour in two different austenitic alloys. One austenitic stainless steel (AISI 316L) and one nickel-base alloy (Alloy 617) have been investigated. Scanning electron microscopy related techniques as electron channelling contrast imaging and electron backscattering diffraction have been used to study the damage and fracture micromechanisms. For both alloys the dominante damage micromech- anisms are slip bands and planar slip interacting with grain bounderies or precipitates causing strain concentrations. The dominante fracture micromechanism when using a slow strain rate at elevated temperature, is microcracks at grain bounderies due to grain boundery embrittlement caused by precipitates. The decrease in strain rate seems to have a small influence on dynamic strain ageing at 650℃. 展开更多
关键词 dynamic strain ageing slow strain rate tensile testing FRACTURE DAMAGE
下载PDF
Effects of Strain Rate on Stress Corrosion of S355 Steel in 3.5% NaCl Solutions
2
作者 金亦富 SHENG Tianyuan +3 位作者 KONG Weicheng ZHANG Ruihong WANG Wenchang 孔德军 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2016年第6期1381-1386,共6页
The stress corrosion of S355 steel in 3.5% NaCl solution under the different strain rates was analyzed with the slow strain rate test(SSRT), the stress corrosion cracking(SCC) behaviors of S355 steel under the dif... The stress corrosion of S355 steel in 3.5% NaCl solution under the different strain rates was analyzed with the slow strain rate test(SSRT), the stress corrosion cracking(SCC) behaviors of S355 steel under the different strain rates in the solution were investigated, and the fracture morphologies and compositions of corrosion products under the different strain rates were analyzed with scanning electron microscopy(SEM) and energy dispersive spectrometerry(EDS), respectively. The experimental results show that the SCC sensitivity index is the highest when the strain rate is 2×10-6, and the medium corrosion is the main reason resulting in the highest SCC sensitivity index. The SCC sensitivity index is the least when the strain rate is 5×10-6, and the stress is the main reason resulting in the stress corrosion. The SCC sensitivity index is the middle when the strain rate is 9×10-6, the interaction of stress and medium is the stress corrosion fracture mechanism. 展开更多
关键词 strain rate slow strain rate test S355 steel stress corrosion fracture morphology
下载PDF
7075铝合金应力腐蚀敏感性的SSRT和电化学测试研究 被引量:27
3
作者 刘继华 李荻 +1 位作者 朱国伟 刘培英 《腐蚀与防护》 CAS 北大核心 2005年第1期6-9,共4页
采用慢应变速率试验(SSRT)研究了7075铝合金的应力腐蚀行为。试验结果表明,外加阳极极化和阴极极化都能增加7075铝合金的应力腐蚀敏感性,即使在弱极化情况下也能显著增加合金的应力腐蚀敏感性。但是,外加极化对于不同热处理状态的7075... 采用慢应变速率试验(SSRT)研究了7075铝合金的应力腐蚀行为。试验结果表明,外加阳极极化和阴极极化都能增加7075铝合金的应力腐蚀敏感性,即使在弱极化情况下也能显著增加合金的应力腐蚀敏感性。但是,外加极化对于不同热处理状态的7075铝合金,其应力腐蚀敏感性增加的程度不同。电极极化对T6状态合金的SCC敏感性的影响显著,而对RRA和T7351状态合金的影响较轻微。随着拉伸应力的增加,7075 RRA铝合金的阳极极化曲线略向正移,滞后环面积扩大,但并不显著。 展开更多
关键词 应力腐蚀 慢应变速率拉伸 7075铝合金
下载PDF
基于SSRT的材料应力腐蚀数据库 被引量:3
4
作者 任呈强 赵远兴 刘丽 《材料导报》 EI CAS CSCD 北大核心 2012年第24期26-29,共4页
采用VB程序语言和Microsoft Office Access数据库管理系统,针对慢应变拉伸实验(SSRT)研究了材料应力腐蚀的结果,设计并建立了应力腐蚀数据库,该数据库包括实验参数输入、实验数据计算和断口图片分析3个模块。通过力学性能指标的计算,依... 采用VB程序语言和Microsoft Office Access数据库管理系统,针对慢应变拉伸实验(SSRT)研究了材料应力腐蚀的结果,设计并建立了应力腐蚀数据库,该数据库包括实验参数输入、实验数据计算和断口图片分析3个模块。通过力学性能指标的计算,依据应力腐蚀敏感性判据和断口形貌特征,将应力腐蚀分为敏感、危险和安全3个水平,获得应力腐蚀体系的材料、环境和力学的关联特征,并将综合分析结果作为案例进行储存管理,以供使用者参考相关数据。 展开更多
关键词 敏感性 慢应变拉伸实验 断口 数据库 案例
下载PDF
低温对铝合金在SSRT过程中裂纹萌生与扩展规律的影响 被引量:2
5
作者 尹元博 杜娟 +5 位作者 李香云 魏子明 周松霖 刘京 王付胜 宋肖肖 《有色金属工程》 CAS 北大核心 2019年第9期24-33,78,共11页
采用一种电化学阻抗谱(EIS)的解析方法,原位研究低温对7A04铝合金在慢应变速率拉伸过程(SSRT)中裂纹萌生与扩展规律的影响。利用扫描电子显微镜(SEM)观察断口形貌,并通过Kramers-Kronig转换验证EIS实验数据的可靠性。结果表明,裂纹的萌... 采用一种电化学阻抗谱(EIS)的解析方法,原位研究低温对7A04铝合金在慢应变速率拉伸过程(SSRT)中裂纹萌生与扩展规律的影响。利用扫描电子显微镜(SEM)观察断口形貌,并通过Kramers-Kronig转换验证EIS实验数据的可靠性。结果表明,裂纹的萌生和扩展过程大致可分为氧化膜溶解、裂纹萌生、动态平衡、裂纹明显扩展四个阶段;温度的降低会改变断裂方式,表现为从混合断裂向脆性穿晶断裂发展;由常温向低温的变化可以有效抑制铝合金在SSRT过程中的裂纹萌生和扩展,具体表现为温度越低对裂纹萌生和扩展的抑制效果越不明显,其中-5℃时抑制效果最强。 展开更多
关键词 低温 7A04铝合金 慢应变速率拉伸 电化学阻抗谱
下载PDF
条形缺陷对L360管线钢环焊缝硫化物应力腐蚀开裂敏感性的影响
6
作者 王洪松 冯大成 +4 位作者 付安庆 苏航 吴明畏 赵果 卓柯 《石油管材与仪器》 2024年第1期87-92,共6页
通过抗硫化物应力腐蚀试验、慢应变速率拉伸试验、氢含量测试等方法研究条形缺陷对H_(2)S环境下L360管线钢环焊缝硫化物应力腐蚀开裂敏感性的影响。结果表明,环焊缝在72%、85%和110%SMYS(最小屈服强度)应力水平下,热影响区出现裂纹且裂... 通过抗硫化物应力腐蚀试验、慢应变速率拉伸试验、氢含量测试等方法研究条形缺陷对H_(2)S环境下L360管线钢环焊缝硫化物应力腐蚀开裂敏感性的影响。结果表明,环焊缝在72%、85%和110%SMYS(最小屈服强度)应力水平下,热影响区出现裂纹且裂纹长度随加载应力增大而增大;条形缺陷环焊缝试样在屈服点后快速发生断裂,其断裂应变(0.024)仅为非缺陷环焊缝试样的21.05%;条形缺陷存在促进氢离子在裂纹尖端聚集从而加剧发生开裂倾向,消氢处理技术可以有效降低氢含量,降低环焊缝抗硫化物应力腐蚀开裂敏感性降低。 展开更多
关键词 L360管线钢 条形缺陷 硫化物应力腐蚀试验 消氢处理 慢应变速率拉伸试验
下载PDF
硅酸锌车间底漆对船体钢在海水中氢脆行为的影响研究
7
作者 安佰孝 马晓 +4 位作者 吕雪松 何其健 郝福耀 鲁统军 侯健 《装备环境工程》 CAS 2024年第6期102-110,共9页
目的 研究硅酸锌车间底漆对船体钢在海水中氢脆行为的影响,为船舶建造涂装工艺提供数据支撑。方法 采用电化学测试、慢应变速率试验(SSRT)、断口微观形貌观察,考察带有硅酸锌车间底漆的船体钢在海水中的氢脆行为。结果 自腐蚀状态下,船... 目的 研究硅酸锌车间底漆对船体钢在海水中氢脆行为的影响,为船舶建造涂装工艺提供数据支撑。方法 采用电化学测试、慢应变速率试验(SSRT)、断口微观形貌观察,考察带有硅酸锌车间底漆的船体钢在海水中的氢脆行为。结果 自腐蚀状态下,船体钢及其涂层试样的SSRT断口均以韧性断裂为主,氢脆系数均小于10%,没有明显的氢脆敏感性。–0.94 V阴极保护状态下,船体钢及其涂层试样的SSRT宏观断口均出现了不同程度的撕裂痕,微观断口出现小解理面特征。以硅酸锌涂层做底漆的试样,撕裂痕以及解理面特征最显著,氢脆系数增大最为明显。当船体钢/硅酸锌/环氧耐磨涂层表面出现破损时,氢脆敏感性系数进一步增大。结论 阴极保护状态下,硅酸锌底漆会增加船体钢在海水中的氢脆敏感性。 展开更多
关键词 船体钢 硅酸锌涂层 车间底漆 慢应变速率试验 阴极保护 氢脆
下载PDF
高温水蒸气环境中TP439不锈钢的应力腐蚀开裂敏感性
8
作者 李富天 刘光明 +3 位作者 刘欢欢 何一鹏 李玉 柳志浩 《表面技术》 EI CAS CSCD 北大核心 2024年第2期71-77,96,共8页
目的 研究TP439不锈钢在高温水蒸气环境中的应力腐蚀开裂行为,并探讨水蒸气和温度对其应力腐蚀开裂敏感性的影响规律。方法 采用慢应变速率拉伸试验方法研究了TP439不锈钢在400~600℃水蒸气环境中的应力腐蚀开裂行为,利用SEM和EDS分析... 目的 研究TP439不锈钢在高温水蒸气环境中的应力腐蚀开裂行为,并探讨水蒸气和温度对其应力腐蚀开裂敏感性的影响规律。方法 采用慢应变速率拉伸试验方法研究了TP439不锈钢在400~600℃水蒸气环境中的应力腐蚀开裂行为,利用SEM和EDS分析试样断口区域的形貌及元素分布。结果 同一应变速率(2×10^(-5) s^(-1))下,随着温度在400~600℃范围内升高,TP439不锈钢在空气和水蒸气环境中的屈服强度、抗拉强度和断裂能均逐渐降低,延伸率逐渐增大。400℃和500℃时,试样在水蒸气环境中的抗拉强度较空气环境中有所降低,而延伸率较空气环境中增大。600℃时试样在水蒸气环境中的力学性能较空气环境中无明显差别。试样在400、500、600℃水蒸气环境中的应力腐蚀开裂敏感性指数分别为0.7%、1.2%和-2.8%,应力腐蚀开裂敏感性较低。试样在400~600℃水蒸气环境中的断口均呈现韧性断裂特征,断口形貌整体由韧窝和微孔组成,颈缩现象显著,断口附近未发现二次裂纹。温度在400~600℃范围内升高时,断口的韧窝特征更加明显,颈缩程度逐渐增大,600℃时断口侧面的氧化膜表面Cr含量明显降低,主要由Fe的氧化物形成。结论 水蒸气对TP439不锈钢的应力腐蚀开裂行为起促进作用。基于应力腐蚀开裂敏感性指数和断口的分析,在应变速率为2×10^(-5) s^(-1)的400~600℃水蒸气环境中,TP439不锈钢的应力腐蚀开裂敏感性较低。 展开更多
关键词 铁素体不锈钢 高温水蒸气 慢应变速率拉伸试验 应力腐蚀开裂 断口形貌
下载PDF
SCC evaluation of a 2297 Al-Li alloy rolled plate using the slow-strain rate technique 被引量:4
9
作者 Kuo ZHAO Jianhua LIU +1 位作者 Mei YU Songmei LI 《Chinese Journal of Aeronautics》 SCIE EI CAS CSCD 2019年第11期2516-2525,共10页
The stress corrosion cracking(SCC) susceptibility of 2297 Al-Li alloy in 1 M Na Cl +0.01 M H2O2 solution(CP solution) and 1 M NaCl + 0.01 M H2O2+ 0.6 M Na2SO4 solution(CPS solution) was investigated by slow-strain rat... The stress corrosion cracking(SCC) susceptibility of 2297 Al-Li alloy in 1 M Na Cl +0.01 M H2O2 solution(CP solution) and 1 M NaCl + 0.01 M H2O2+ 0.6 M Na2SO4 solution(CPS solution) was investigated by slow-strain rate tests at various strain rates ranging from 10-5s(-1) to 10-7s-1. The roles of H2O2 and SO42-in the corrosion process were estimated by potentiodynamic polarization and electrochemical impedance spectroscopy. 2297 Al-Li alloy does not fracture ascribed to SCC in CP solution, while it undergoes SCC in CPS solution. In CPS solution,with a decreasing strain rate from 10-5s(-1) to 10-7s-1, the SCC susceptibility firstly rises and then declines exhibiting a peak value at a strain rate of 10-6s-1. H2O2 promotes the active dissolution while SO42- lowers the corrosion rate. The SCC fracture is associated with a decline in the dissolution rate of the crack tip by SO42-, which leads to stress concentration. In CPS solution, a reduction in the local dissolution rate of the crack tip leads to stress concentration, resulting in SCC fracture.As the preferred initiation site for a crack, pits also show a noteworthy effect on SCC of 2297 Al-Li alloy. 展开更多
关键词 Al-Li alloy DISSOLUTION Electrochemical behavior slow strain rate testing Stress corrosion cracking
原文传递
不同温度下6082铝合金的抗应力腐蚀性能
10
作者 王建军 罗先甫 +3 位作者 刘煜 王佳 孙绪鲁 查小琴 《理化检验(物理分册)》 CAS 2024年第3期16-19,22,共5页
采用慢应变速率拉伸试验方法研究了6082铝合金板材在不同温度下的抗应力腐蚀性能,采用光学显微镜和透射电镜观察其显微组织,采用扫描电镜对其进行断口分析。结果表明:6082铝合金板材在70℃,3.5%(体积分数)NaCl溶液中的应力腐蚀敏感性指... 采用慢应变速率拉伸试验方法研究了6082铝合金板材在不同温度下的抗应力腐蚀性能,采用光学显微镜和透射电镜观察其显微组织,采用扫描电镜对其进行断口分析。结果表明:6082铝合金板材在70℃,3.5%(体积分数)NaCl溶液中的应力腐蚀敏感性指数为6.6%,在50℃,3.5%(体积分数)NaCl溶液中的应力腐蚀敏感性指数为2.3%;试样断口均无应力腐蚀特征,合金晶内析出了弥散分布的细小Mg2Si相,晶界析出了不连续分布的Mg2Si相,不能形成连续的沿晶腐蚀通道,试样表现为较好的抗应力腐蚀性能;温度升高使试样在腐蚀溶液中的抗拉强度下降幅度较大,试样在70℃下的应力腐蚀敏感性指数偏高。 展开更多
关键词 6082铝合金 慢应变速率拉伸试验 应力腐蚀敏感性指数 钝化膜
下载PDF
7B04铝合金应力腐蚀敏感性研究 被引量:12
11
作者 刘远勇 张晓云 +2 位作者 裴和中 陆峰 高健 《材料工程》 EI CAS CSCD 北大核心 2010年第2期33-36,41,共5页
利用慢应变速率拉伸应力腐蚀实验方法研究7B04铝合金的应力腐蚀开裂敏感性。研究温度、腐蚀介质、电化学极化对应力腐蚀敏感性的影响,结果表明:随温度的升高7B04铝合金的应力腐蚀开裂敏感性增强;溶液的腐蚀性越强,7B04铝合金的应力腐蚀... 利用慢应变速率拉伸应力腐蚀实验方法研究7B04铝合金的应力腐蚀开裂敏感性。研究温度、腐蚀介质、电化学极化对应力腐蚀敏感性的影响,结果表明:随温度的升高7B04铝合金的应力腐蚀开裂敏感性增强;溶液的腐蚀性越强,7B04铝合金的应力腐蚀开裂敏感性越大;无论是阳极极化还是阴极极化都会增加7B04铝合金的应力腐蚀开裂敏感性。 展开更多
关键词 7B04铝合金 应力腐蚀开裂SCC 慢应变速率拉伸实验
下载PDF
拉伸变形对304不锈钢应力腐蚀的影响 被引量:19
12
作者 许淳淳 张新生 胡钢 《材料研究学报》 EI CAS CSCD 北大核心 2003年第3期310-314,共5页
研究了在-70℃和180℃拉伸变形对304不锈钢应力腐蚀的影响,结果表明,随着拉伸变形量的增加,180℃拉伸变形的304不锈钢在42%沸腾MgCl_2溶液中应力腐蚀破裂敏感性逐渐减小,而在-70℃拉伸变形的304不锈钢在42%沸腾MgCl_2溶液中应力腐蚀... 研究了在-70℃和180℃拉伸变形对304不锈钢应力腐蚀的影响,结果表明,随着拉伸变形量的增加,180℃拉伸变形的304不锈钢在42%沸腾MgCl_2溶液中应力腐蚀破裂敏感性逐渐减小,而在-70℃拉伸变形的304不锈钢在42%沸腾MgCl_2溶液中应力腐蚀破裂敏感性经历了一个从减小到增大的过程。马氏体相的存在导致304不锈钢在42%沸腾MgCl_2溶液中应力腐蚀破裂敏感性增大。 展开更多
关键词 材料失效与保护 应力腐蚀破裂敏感性 慢应变速率方法(ssrt) 304不锈钢 马氏体相
下载PDF
电化学极化对2D12铝合金应力腐蚀断裂敏感性的影响 被引量:7
13
作者 张晓云 张成国 +2 位作者 霍乾明 郭孟秋 高健 《腐蚀与防护》 CAS 北大核心 2009年第8期531-533,共3页
利用慢应变速率拉伸应力腐蚀试验方法评价了高强度铝合金2D12/T4的应力腐蚀敏感性,研究了电化学极化对其应力腐蚀敏感性的影响。结果表明2D12铝合金具有一定的应力腐蚀敏感性,阳极极化对2D12铝合金应力腐蚀敏感性的影响要比阴极极化显著... 利用慢应变速率拉伸应力腐蚀试验方法评价了高强度铝合金2D12/T4的应力腐蚀敏感性,研究了电化学极化对其应力腐蚀敏感性的影响。结果表明2D12铝合金具有一定的应力腐蚀敏感性,阳极极化对2D12铝合金应力腐蚀敏感性的影响要比阴极极化显著。2D12铝合金的应力腐蚀开裂机制以阳极溶解为主。 展开更多
关键词 铝合金 应力腐蚀 慢应变拉伸
下载PDF
激光冲击对X80管线钢焊接接头应力腐蚀的影响 被引量:6
14
作者 孔德军 龙丹 +1 位作者 吴永忠 周朝政 《建筑材料学报》 EI CAS CSCD 北大核心 2012年第4期484-489,共6页
利用激光冲击波对X80管线钢焊接接头进行了表面改性处理,通过慢拉伸试验分析了X80管线钢焊接接头在NACE溶液(不含H2S和含饱和H2S)的H2S应力腐蚀开裂(SCC)行为,研究了经激光冲击处理后焊接接头表面细化的晶粒和残余应力对H2S应力腐蚀的... 利用激光冲击波对X80管线钢焊接接头进行了表面改性处理,通过慢拉伸试验分析了X80管线钢焊接接头在NACE溶液(不含H2S和含饱和H2S)的H2S应力腐蚀开裂(SCC)行为,研究了经激光冲击处理后焊接接头表面细化的晶粒和残余应力对H2S应力腐蚀的影响机理.结果表明:激光冲击处理可改善焊接接头的表面质量,形成强化层,产生晶粒细化和残余压应力,获得细小均匀的针状铁素体组织,因大量晶粒承受氢压,可显著提高材料的临界应力值。应力腐蚀敏感指数ISCC比原始状态下降了5.84%,提高了X80管线钢焊接接头抗SCC的性能.激光冲击处理使X80管线钢焊接接头表面粗糙度有所上升,在一定程度上又降低了X80管线钢焊接接头SCC抗力. 展开更多
关键词 激光冲击处理 X80管线钢 焊接接头 应力腐蚀 慢拉伸试验
下载PDF
浓度和温度对316L不锈钢在NaOH溶液中应力腐蚀开裂行为的影响 被引量:12
15
作者 姜勇 巩建鸣 周荣荣 《腐蚀与防护》 CAS 北大核心 2008年第12期749-751,共3页
采用慢应变速率拉伸试验(简称SSRT),对316L不锈钢在高温NaOH溶液中的应力腐蚀开裂行为进行了试验研究,结果表明在较高温度下,316L不锈钢在低浓度的NaOH溶液中也具有明显的应力腐蚀开裂敏感性。
关键词 不锈钢 应力腐蚀开裂(SCC) 慢应变速率拉伸试验(ssrt) NAOH溶液
下载PDF
激光冲击对X70焊接接头慢拉伸电化学腐蚀的影响 被引量:6
16
作者 孔德军 吴永忠 龙丹 《材料科学与工艺》 EI CAS CSCD 北大核心 2012年第1期139-143,共5页
为了改善X70管线钢焊接接头慢拉伸电化学腐蚀性能,用激光冲击波对X70管线钢焊接接头表面进行强化处理.采用慢应变速率拉伸法分析了X70管线钢焊接接头,在不同H2S浓度的NACE溶液(0.5%HAC+5%NaCl)中电化学腐蚀行为,测试了激光冲击处理前后... 为了改善X70管线钢焊接接头慢拉伸电化学腐蚀性能,用激光冲击波对X70管线钢焊接接头表面进行强化处理.采用慢应变速率拉伸法分析了X70管线钢焊接接头,在不同H2S浓度的NACE溶液(0.5%HAC+5%NaCl)中电化学腐蚀行为,测试了激光冲击处理前后X70管线钢焊接接头腐蚀电位,讨论了激光冲击处理对X70管线钢焊接接头腐蚀电位和断口形貌的影响.实验结果表明,激光冲击处理改善了X70管线钢焊接接头腐蚀性能,其SCC敏感性指数Iscc降低了6%.经激光冲击处理后试样自然腐蚀电位正移,极化电阻逐渐增大,其耐蚀性比原始状态有所提高. 展开更多
关键词 激光冲击处理 X70管线钢 焊接接头 慢拉伸 电化学腐蚀
下载PDF
应变速率及环境介质对Zn-Cu-Ti合金应力腐蚀行为的影响 被引量:7
17
作者 王彦红 肖来荣 +2 位作者 耿占吉 饶博 康思清 《腐蚀与防护》 CAS 北大核心 2013年第5期410-412,416,共4页
采用慢应变速率拉伸试验(SSRT)、扫描电镜(SEM)等方法研究了挤压态Zn-1.0Cu-0.2Ti(wt%)合金在空气、自来水及3.5%NaCl溶液中的应力腐蚀开裂(SCC)行为及应变速率对合金SCC行为的影响。结果表明,应变速率为1×10-6s-1时,合金的SCC敏... 采用慢应变速率拉伸试验(SSRT)、扫描电镜(SEM)等方法研究了挤压态Zn-1.0Cu-0.2Ti(wt%)合金在空气、自来水及3.5%NaCl溶液中的应力腐蚀开裂(SCC)行为及应变速率对合金SCC行为的影响。结果表明,应变速率为1×10-6s-1时,合金的SCC敏感性最大;在1×10-6s-1的应变速率下,合金在自来水与3.5%NaCl溶液中的SCC敏感性比空气中弱。 展开更多
关键词 Zn-Cu-Ti合金 慢应变速率拉伸试验(ssrt) 应力腐蚀开裂(scc)
下载PDF
SPV50Q高强钢焊接接头在湿H_2S环境下的开裂敏感性研究 被引量:4
18
作者 唐建群 巩建鸣 +1 位作者 张显成 涂善东 《机械强度》 EI CAS CSCD 北大核心 2007年第1期97-102,共6页
具有较高强度和良好韧性的SPV50Q钢常用于制造液化石油气(liquefiedpetroleumgas,LPG)球罐,球罐通过焊接制造后一般不经过焊后热处理,因此在焊接接头处将有焊接残余应力存在。服役经历和现场检测表明,较高H2S浓度和焊接残余应力将会导... 具有较高强度和良好韧性的SPV50Q钢常用于制造液化石油气(liquefiedpetroleumgas,LPG)球罐,球罐通过焊接制造后一般不经过焊后热处理,因此在焊接接头处将有焊接残余应力存在。服役经历和现场检测表明,较高H2S浓度和焊接残余应力将会导致材料产生环境失效如氢鼓泡(hydrogenblistering,HB)或氢致开裂(hydrogen-inducedcracking,HIC)、硫化物应力腐蚀开裂(sulfidestresscorrosioncracking,SSCC)以及应力诱导氢致开裂(stress-orientedhydrogeninducedcracking,SOHIC)。文中通过1×10-6s-1的慢应变速率拉伸试验,对手工电弧焊焊接的SPV50Q焊接接头在不同浓度H2S水溶液中的开裂敏感性以及开裂特征进行研究。试验结果表明,SSCC和HIC发生在靠近焊接接头热影响区的母材上,不同温度下的焊后热处理将降低材料的应力腐蚀开裂敏感性,实施正确焊后热处理可提高SPV50Q焊接接头抵抗SSCC或HIC能力,而不降低钢的力学性能尤其是韧性。 展开更多
关键词 高强钢 硫化物应力腐蚀开裂 氢致开裂 H2S浓度 慢应变速率试验 焊后热处理
下载PDF
阴极保护电位对E460钢氢脆敏感性的影响 被引量:4
19
作者 陈祥曦 马力 +2 位作者 赵程 张海兵 许立坤 《腐蚀与防护》 CAS 北大核心 2015年第11期1026-1029,1071,共5页
采用慢应变速率试验(SSRT)和电化学方法结合断口扫描电镜观察,研究了阴极保护电位对E460钢在海水中氢脆敏感性的影响。结果表明,随着阴极保护电位负移,E460钢在海水中的氢脆敏感性增加,阴极保护电位为-0.95V(vs.SCE,下同)时,拉伸试样出... 采用慢应变速率试验(SSRT)和电化学方法结合断口扫描电镜观察,研究了阴极保护电位对E460钢在海水中氢脆敏感性的影响。结果表明,随着阴极保护电位负移,E460钢在海水中的氢脆敏感性增加,阴极保护电位为-0.95V(vs.SCE,下同)时,拉伸试样出现脆性解理断裂特征,电位为-1.05V时,E460钢断口呈脆性断裂特征。 展开更多
关键词 氢脆 阴极保护 慢应变速率试验(ssrt) E460钢
下载PDF
17-4PH不锈钢的析氢行为 被引量:4
20
作者 张海兵 马力 +2 位作者 闫永贵 程文华 袁亚民 《腐蚀与防护》 CAS 北大核心 2016年第4期317-320,共4页
采用电化学测试的方法评价了两种强度的17-4PH不锈钢在海水中的阴极极化行为;采用充氢试验研究了两种强度的17-4PH不锈钢在-1.1V(SCE,下同)电位下阴极极化15d后的含氢量;采用慢应变速率试验研究了两种强度17-4PH不锈钢在充氢后的氢脆系... 采用电化学测试的方法评价了两种强度的17-4PH不锈钢在海水中的阴极极化行为;采用充氢试验研究了两种强度的17-4PH不锈钢在-1.1V(SCE,下同)电位下阴极极化15d后的含氢量;采用慢应变速率试验研究了两种强度17-4PH不锈钢在充氢后的氢脆系数。结果表明:两种强度的17-4PH不锈钢在海水中的析氢转变电位均在-0.90V左右;低强度不锈钢的氢质量分数约为2.55×10^(-4)%,而高强度不锈钢的氢质量分数则高达6.84×10^(-4)%;试样充氢后,高强度不锈钢的脆性明显增加,而低强度不锈钢的脆性增加不明显,高强度不锈钢的氢脆系数远超过25%,此时材料已存在氢脆危险,而低强度不锈钢的氢脆系数约为18%左右,尚处于氢脆安全区。 展开更多
关键词 17-4PH不锈钢 析氢 电化学测试 慢应变速率试验
下载PDF
上一页 1 2 10 下一页 到第
使用帮助 返回顶部