The use of coral aggregate concrete(CAC)as a novel construction material has attracted significant attention for the construction of reef engineering structures.To investigate the static splitting-tensile behaviors of...The use of coral aggregate concrete(CAC)as a novel construction material has attracted significant attention for the construction of reef engineering structures.To investigate the static splitting-tensile behaviors of CAC under the influence of two factors,namely specimen geometry and bearing strip size,a three-dimensional(3D)mesoscale modeling approach with consideration for aggregate randomness in shape and distribution was adopted in this study.We established 12 different specimen models with two specimen shapes(i.e.,a cube with an edge length of 150 mm and a cylinder with dimensions ofφ150 mm×300 mm)and six strip widths(i.e.,6,9,12,15,18,and 20 mm)for calculation.The effects of specimen geometry and strip width on the splitting-tensile properties of CAC,such as failure processes,final failure patterns,and splitting-tensile strength(fst),are analyzed and discussed systematically.The results indicate the high reliability of the developed mesoscale modeling approach and reveal the optimal computational parameters for simulating and predicting the splitting-tensile properties of CAC.The fstvalues of CAC are associated with both the specimen geometry and width of the bearing strip.The fstvalues of the cube model are slightly higher than those of the cylinder model for the same bearing strip size,representing geometry effects that can be explained by differences in fracture area.Additionally,the fstvalue of CAC gradually increases with the relative width of the bearing strip ranging from 0.04 to 0.13.Based on the elastic solution theory,the variation area of CAC fstvalues with the relative width of the bearing strip was determined preliminarily,which has great significance for studying the tensile performance of CAC.展开更多
Tests were carried out to study the strength deterioration of concrete cooled in air or by water after sub-high temperature at different level and varying with cycles. It is proved that the cross-shaped cracks turned ...Tests were carried out to study the strength deterioration of concrete cooled in air or by water after sub-high temperature at different level and varying with cycles. It is proved that the cross-shaped cracks turned up and extended little by little on the surface of specimen subjected to repeat sub-high temperature, the splitting failure is characterized by cross-shaped cracks after 30 cycles, the concrete strengths decrease rapidly at early stage and to be steady subsequently with the increase of the temperature cycles, the splitting-tensile strength is more sensitive to temperature cycles than the compressive strength, the decline of concrete strength is mainly controlled by the maximum temperature having reached, the ultrasonic velocity in concrete is also declined. On the basis of test results, the mechanisms of sub-high temperature to the strength deterioration of concrete are analyzed.The formulas for calculating the compressive and splitting-tensile strength of concrete relating to the variation of temperature are proposed.展开更多
基金financial support from the National Natural Science Foundation of China(52178190,51878350,11832013,51678304,and 52078250)the Science and Technology on Near-Surface Detection Laboratory pre-research Fund(6142414200505)+1 种基金the Interdisciplinary Innovation Foundation for Graduates,Nanjing University of Aeronautics and Astronautics(NUAA)Grant(KXKCXJJ202005)The support provided by the China Scholarship Council(202006830096)during a visit of Zhangyu Wu to University College London is also sincerely acknowledged。
文摘The use of coral aggregate concrete(CAC)as a novel construction material has attracted significant attention for the construction of reef engineering structures.To investigate the static splitting-tensile behaviors of CAC under the influence of two factors,namely specimen geometry and bearing strip size,a three-dimensional(3D)mesoscale modeling approach with consideration for aggregate randomness in shape and distribution was adopted in this study.We established 12 different specimen models with two specimen shapes(i.e.,a cube with an edge length of 150 mm and a cylinder with dimensions ofφ150 mm×300 mm)and six strip widths(i.e.,6,9,12,15,18,and 20 mm)for calculation.The effects of specimen geometry and strip width on the splitting-tensile properties of CAC,such as failure processes,final failure patterns,and splitting-tensile strength(fst),are analyzed and discussed systematically.The results indicate the high reliability of the developed mesoscale modeling approach and reveal the optimal computational parameters for simulating and predicting the splitting-tensile properties of CAC.The fstvalues of CAC are associated with both the specimen geometry and width of the bearing strip.The fstvalues of the cube model are slightly higher than those of the cylinder model for the same bearing strip size,representing geometry effects that can be explained by differences in fracture area.Additionally,the fstvalue of CAC gradually increases with the relative width of the bearing strip ranging from 0.04 to 0.13.Based on the elastic solution theory,the variation area of CAC fstvalues with the relative width of the bearing strip was determined preliminarily,which has great significance for studying the tensile performance of CAC.
基金Funded by Outstanding Youth Science Foundation of Henan Province of China (No. 04120002300)
文摘Tests were carried out to study the strength deterioration of concrete cooled in air or by water after sub-high temperature at different level and varying with cycles. It is proved that the cross-shaped cracks turned up and extended little by little on the surface of specimen subjected to repeat sub-high temperature, the splitting failure is characterized by cross-shaped cracks after 30 cycles, the concrete strengths decrease rapidly at early stage and to be steady subsequently with the increase of the temperature cycles, the splitting-tensile strength is more sensitive to temperature cycles than the compressive strength, the decline of concrete strength is mainly controlled by the maximum temperature having reached, the ultrasonic velocity in concrete is also declined. On the basis of test results, the mechanisms of sub-high temperature to the strength deterioration of concrete are analyzed.The formulas for calculating the compressive and splitting-tensile strength of concrete relating to the variation of temperature are proposed.