Development of SA-533 Type B CL. 1+SA-240 Type 304L roll-bonded clad steel plate for safety injection tank of CAP1400 nuclear power plant 被引量:3
1
作者 HOU Hong ZHANG Hanqian +1 位作者 YUAN Xiangqian DING Jianhua 《Baosteel Technical Research》 CAS 2017年第1期18-25,共8页
Aiming to meet the demand of the country' s nuclear demonstration project on the CAP1400 nuclear power plant, Baosteel uses the roll-bonding technology and develops the SA-533 Type B CL. 1 + SA-240 Type 304L high-st... Aiming to meet the demand of the country' s nuclear demonstration project on the CAP1400 nuclear power plant, Baosteel uses the roll-bonding technology and develops the SA-533 Type B CL. 1 + SA-240 Type 304L high-strength and high-toughness clad steel plate with a shear strength of over 310 MPa for the nuclear power plant' s safety injection tank. The properties of the quenched and tempered and the simulated post-weld heat treatment states are systematically studied herein through a comprehensive inspection and evaluation of the composition,microstructure,and properties of the clad steel plate. The results show that the bonding interface has high shear strength and that the base metal has high strength and good toughness at low temperatures. Hence, the performance fully meets the technical requirements of the CAP1400 nuclear power plant' s safety injection tank in the country' s nuclear demonstration project. The roll-bonded clad steel plate can be used to manufacture the safety injection tank of the CAP1400 nuclear power plant. 展开更多
关键词 CAP1400 nuclear power plant safety injection tank sa-533 Type B CL. 1 sa-240 Type 304Lrolling clad steel plate quenched and tempered simulated post-weld heat treatment property
下载PDF
SA-387钢冷压开裂原因分析 被引量:1
2
作者 姜树立 姜艳 王君 《应用科技》 CAS 2005年第4期60-61,共2页
某锅炉厂在冷压制气化炉用SA-387钢板时,该钢发生了开裂.对断裂断口进行了扫描电镜和能谱分析,找出了造成SA-387钢板压制开裂的原因是在钢板内部有密集的大块非金属夹杂物存在;这些夹杂物很有可能是来自于连铸钢的保护渣,这些皮下夹杂... 某锅炉厂在冷压制气化炉用SA-387钢板时,该钢发生了开裂.对断裂断口进行了扫描电镜和能谱分析,找出了造成SA-387钢板压制开裂的原因是在钢板内部有密集的大块非金属夹杂物存在;这些夹杂物很有可能是来自于连铸钢的保护渣,这些皮下夹杂物富集在钢的局部,在后续的轧制过程中,沿轧制方向被轧制呈条带状,最终可能会贯穿整块钢板,形成一条极危险的条状夹杂物区,因此在钢板冷压制过程中出现开裂. 展开更多
关键词 sa-387钢板 非金属夹杂物 失效分析 断裂