A new cement free iron trough castable was prepared with dense corundum and silicon carbide as the main raw materials and submicron SiO_(2) powder(d_(50)=0.242μm,SiO_(2)=99.9 mass%)as the binder.The effect of the sub...A new cement free iron trough castable was prepared with dense corundum and silicon carbide as the main raw materials and submicron SiO_(2) powder(d_(50)=0.242μm,SiO_(2)=99.9 mass%)as the binder.The effect of the submicron SiO_(2) powder addition(3%,4%,5%,6%,7%,8%,and 9%,by mass,respectively)on the properties of the prepared castables was studied.The working mechanism of submicron SiO_(2) powder was analyzed from the perspective of the particle size distribution and infrared absorption spectrum.The results show that:(1)cement free iron trough castables can be prepared using submicron SiO_(2) powder alone as the binder;(2)compared with traditional castables,the cement free castables have made a breakthrough in the water addition and hot modulus of rupture.The optimal submicron SiO_(2) powder addition is 4%-6%.展开更多
The nanometer particles of TiO_2 and TiO_2/SiO_2 oxides wereprepared by sol-gel supercritical fluid drying method. The propertiesof TiO_2 and TiO_2/SiO_2 were characterized by means of BET(Brunner-Emmett- Teller metho...The nanometer particles of TiO_2 and TiO_2/SiO_2 oxides wereprepared by sol-gel supercritical fluid drying method. The propertiesof TiO_2 and TiO_2/SiO_2 were characterized by means of BET(Brunner-Emmett- Teller method), TEM (transmission electronmicroscopy), SEM (scanning electron microscopy), XRD (X-ray diffrac-tion) and FTIR (Fourier transform-infrared) techniques. The effectsof different preparation route, prehydrolysis and non-prehydrolysis,on the properties of TiO_2/SiO_2 oxide were also examined.展开更多
基金support from the National Natural Science Foundation of China(NSFC,No.51804233)。
文摘A new cement free iron trough castable was prepared with dense corundum and silicon carbide as the main raw materials and submicron SiO_(2) powder(d_(50)=0.242μm,SiO_(2)=99.9 mass%)as the binder.The effect of the submicron SiO_(2) powder addition(3%,4%,5%,6%,7%,8%,and 9%,by mass,respectively)on the properties of the prepared castables was studied.The working mechanism of submicron SiO_(2) powder was analyzed from the perspective of the particle size distribution and infrared absorption spectrum.The results show that:(1)cement free iron trough castables can be prepared using submicron SiO_(2) powder alone as the binder;(2)compared with traditional castables,the cement free castables have made a breakthrough in the water addition and hot modulus of rupture.The optimal submicron SiO_(2) powder addition is 4%-6%.
基金Supported by PetroChina Company Limited (990801-21-2).
文摘The nanometer particles of TiO_2 and TiO_2/SiO_2 oxides wereprepared by sol-gel supercritical fluid drying method. The propertiesof TiO_2 and TiO_2/SiO_2 were characterized by means of BET(Brunner-Emmett- Teller method), TEM (transmission electronmicroscopy), SEM (scanning electron microscopy), XRD (X-ray diffrac-tion) and FTIR (Fourier transform-infrared) techniques. The effectsof different preparation route, prehydrolysis and non-prehydrolysis,on the properties of TiO_2/SiO_2 oxide were also examined.