Natural durability of two plantation woods, Chinese fir and I-214 poplar, was investigated thoroughly by three test- ing methods, namely an accelerated laboratory decay test, a fungus cellar test and a field test. Af...Natural durability of two plantation woods, Chinese fir and I-214 poplar, was investigated thoroughly by three test- ing methods, namely an accelerated laboratory decay test, a fungus cellar test and a field test. After the decay test using Postia pla- centa and Trametes versicolor, Chinese fir and the I-214 poplar showed 34% and 69% of mass loss, respectively, indicating they should be classified as slightly durable and non-durable wood. This conclusion was confirmed by the fungus cellar test and the field test. Like the performance in the decay test, I-214 poplar showed no resistance to termites either in the laboratory or in the field, whereas Chinese fir would be classified as moderately resistant.展开更多
基金Supported by Sino-Japanese Technical Cooperation Project Titled "Studies on Chinese Plantation Wood" (JICA PROJECT/033-1418-E-O)
文摘Natural durability of two plantation woods, Chinese fir and I-214 poplar, was investigated thoroughly by three test- ing methods, namely an accelerated laboratory decay test, a fungus cellar test and a field test. After the decay test using Postia pla- centa and Trametes versicolor, Chinese fir and the I-214 poplar showed 34% and 69% of mass loss, respectively, indicating they should be classified as slightly durable and non-durable wood. This conclusion was confirmed by the fungus cellar test and the field test. Like the performance in the decay test, I-214 poplar showed no resistance to termites either in the laboratory or in the field, whereas Chinese fir would be classified as moderately resistant.