Repair welding of AA 6082-T6 joints was carried out using ER 4043 filler through the TIG welding process with or without pulsed current.Microstructure and mechanical characteristics of the joints before and after repa...Repair welding of AA 6082-T6 joints was carried out using ER 4043 filler through the TIG welding process with or without pulsed current.Microstructure and mechanical characteristics of the joints before and after repairing were investigated by examining macrostructure,microstructure,and distributions of porosity in the weld metal(WM),and by hardness,tensile,and bending tests.We observed that the welding current,phase transformations in heat-affected zone(HAZ)and porosity introduced in the WM during welding influence on its mechanical properties in sequence.The experimental results showed that the bead width and penetration as well as size of pores in the joints were mainly influenced by the welding currents.The sound joints were obtained at a welding current of 140 A with or without pulsed current when welding speed and gas flow rate were set at 20 cm·min-1 and 15 L·min-1,respectively.Among them,the decrease in mechanical properties of repair weld(RW)was directly related to the phase transformations in the over-ageing zone due to the double welding thermal cycles and elevated distribution of porosity in the WM.In addition,it was observed that the comparatively smaller grain size and lower porosity in WM of the RW produced by pulsed TIG welding gave a positive effect on its mechanical properties.展开更多
A device for superimposing vibration on workpiece in both horizontal and vertical directions during tungsten-arc inert gas (TIG) welding was developed, with maximum power output of 2 kW at frequency of 15 kHz. AZ31 ...A device for superimposing vibration on workpiece in both horizontal and vertical directions during tungsten-arc inert gas (TIG) welding was developed, with maximum power output of 2 kW at frequency of 15 kHz. AZ31 sheets with thickness of I and 3 mm were used in the vibratory welding. Microstructures along with the mechanical properties of the weld joints under different vibrating conditions (vibration direction, vibration amplitude and groove angle) were examined. It is observed that the grain size in welding zone decreases remarkably with the application of vibration, while the amount of second phase β-Mg_17Al_12 within the zone decreases slightly; meanwhile, microhardness of the weld joints, macroscopic tensile strength and elongation of the weldment increase. Vibration, especially the one along vertical direction, has more impact on the performance of the thick weldments. Influence of vibration on mierostructure and mechanical properties of weldments is affected by wave energy transferring in the melt and depends on the processing and geometric parameters including amplitude and direction of vibration, thickness, and groove angles.展开更多
采用TIG(Tungsten inert gas welding,TIG)焊对FeCrAl合金管同质材料进行焊接,通过扫描电子显微镜、透射电子显微镜及能谱仪等手段研究了焊后接头的显微组织特征、焊后接头不同区域氧化物颗粒的分布情况及焊接接头的力学性能。FeCrAl合...采用TIG(Tungsten inert gas welding,TIG)焊对FeCrAl合金管同质材料进行焊接,通过扫描电子显微镜、透射电子显微镜及能谱仪等手段研究了焊后接头的显微组织特征、焊后接头不同区域氧化物颗粒的分布情况及焊接接头的力学性能。FeCrAl合金TIG焊通过填充等成分的FeCrAl合金丝材进行焊接,焊后焊接接头主要由焊缝区、热影响区及母材组成。其中焊缝区为粗大的铁素体组织,热影响区为细小的等轴晶组织。焊缝区的Y_(2)O_(3)氧化物颗粒发生了明显粗化并与基体反应生成复合氧化物Y_(3)Al_(5)O_(12)。TIG焊焊接FeCrAl合金管热处理后,焊接接头最大抗拉强度值为530 MPa,约为母材强度的80.8%,可以实现大口径、大壁厚的FeCrAl合金管材的对接接头的力学性能要求。展开更多
Tungsten inert gas weld was carried out on super-light magnesium-lithium alloy plates with a thickness of 2 mm, using argon gas as a protecting atmosphere. The microstructure and mechanical properties of the welded jo...Tungsten inert gas weld was carried out on super-light magnesium-lithium alloy plates with a thickness of 2 mm, using argon gas as a protecting atmosphere. The microstructure and mechanical properties of the welded joints were investigated. The results indicate that the microstructure in the fusion zone is fine, and the microstructure in the heat-affected zone is coarser than the parent metal. The tensile strength of the welded joint is about 84% that of the parent metal. The fracture occurs in a mixed type of toughness and brittleness in the heat-affected zone. During the welding process, aluminum and cerium are enriched at grain boundaries in the fusion zone.展开更多
The ultrasonic assisted tungsten inert gas (U-TIG) welding is a newly developed arc welding method, which is aimed at improving the weld quality and efficiency. TIG welding and U-TIG welding of 2014 aluminum alloy w...The ultrasonic assisted tungsten inert gas (U-TIG) welding is a newly developed arc welding method, which is aimed at improving the weld quality and efficiency. TIG welding and U-TIG welding of 2014 aluminum alloy with 5 mm thickness were experimentally carried out in this paper. The microstructure and porosity of welded joints were analyzed. Compared with conventional TIG welding, the columnar crystals are changed into equiaxed crystals at the centre of weld zone and the grain of fusion zone in U-TIG welding is refined and equiaxed. The porosities of joint decrease after the ultrasonic was applied on the arc. The mechanism of crystal grain refinement is discussed in this paper and the reasons of porosity decrease in U-TIG welded joint may be due to the effect of acoustic streaming and cavitation, which need further research.展开更多
This paper deals with a novel dual shield TIG welding method named gas pool coupled activating TIG( GPCA-TIG)welding. The welding method divides the shielding gas into two layers. Inert gas such as Ar is adopted as th...This paper deals with a novel dual shield TIG welding method named gas pool coupled activating TIG( GPCA-TIG)welding. The welding method divides the shielding gas into two layers. Inert gas such as Ar is adopted as the inner layer gas to protect the tungsten electrode and the molten pool metal. Pure O_2,N_2 or mixture of them are used as the outer layer gas to increase the weld penetration and improve the low temperature toughness of weld metal. Through analyzing the interaction between outer gas and arc and the distributions and existing forms of oxygen and nitrogen elements,the transfer behaviors of nitrogen and oxygen from arc to pool were investigated. The results show that,the interaction between the outer gas and arc plasma makes the arc slightly constrict. The incoming oxygen enriches on the molten pool surface and exists in the form of iron oxide,chromium oxide,manganese oxide and silicon oxygen compounds. The incoming nitrogen evenly distributes in the molten pool and exists in the form of nitrogen atom.展开更多
Three-dimensional finite element model was established to simulate temperature fields of T-joint titanium sheets during TIG welding with finite element method (FEM) software. Temperature dependent material propertie...Three-dimensional finite element model was established to simulate temperature fields of T-joint titanium sheets during TIG welding with finite element method (FEM) software. Temperature dependent material properties and the effect of latent heat were considered. A technique of element birth and death was used to simulate the process of welded metal filling. Dynamic variation process of temperature fields during T1G welding was achieved. The simulated results agreed well with the measured results.展开更多
In order to realize automatic control of the width of weld pool, a visual sensor system for the width of weld pool detection is developed. By initiative arc light, the image of copper plate weld pool is taken back of ...In order to realize automatic control of the width of weld pool, a visual sensor system for the width of weld pool detection is developed. By initiative arc light, the image of copper plate weld pool is taken back of the torch through the process of weakening and filtering arc light. In order to decrease the time of processing video signals, analog circuit is applied in the processing where video signals is magnified, trimmed and processed into binary on the datum of dynamic average value, therefore the waveform of video signals of weld pool is obtained. The method that is used for detecting the width of weld pool is established. Results show that the vision sensing method for real-time detecting weld pool width to copper-clad aluminum wire TIG welding is feasible. The response cycle of this system is no more than 50 ms, and the testing precision is less than 0. 1 mm.展开更多
Methods of arc length control and visual image based weld detection for precision pulse TIG welding were investigated. With a particular all hardware circuit, arc voltage during peak current stage is sampled and inte...Methods of arc length control and visual image based weld detection for precision pulse TIG welding were investigated. With a particular all hardware circuit, arc voltage during peak current stage is sampled and integrated to indicate arc length, deviation of arc length and adjusting parameters are calculated and output to drive a step motor directly. According to the features of welding image grabbed with CCD camera, a special algorithm was developed to detect the central line of weld fast and accurately. Then an application system were established, whose static arc length error is ±0.1 mm with 20 A average current and 1 mm given arc length, static detection precision of weld is 0.01 mm , processing time of each image is less than 120 ms . Precision pulse TIG welding of some given thin stainless steel components with complicated curved surface was successfully realized.展开更多
The automatic tungsten-inert gas welding(ATIGW) of AZ31 Mg alloys was performed using a six-axis robot. The evolution of the microstructure and texture of the AZ31 auto-welded joints was studied by optical microscop...The automatic tungsten-inert gas welding(ATIGW) of AZ31 Mg alloys was performed using a six-axis robot. The evolution of the microstructure and texture of the AZ31 auto-welded joints was studied by optical microscopy, scanning electron microscopy, energy-dispersive X-ray spectroscopy, and electron backscatter diffraction. The ATIGW process resulted in coarse recrystallized grains in the heat affected zone(HAZ) and epitaxial growth of columnar grains in the fusion zone(FZ). Substantial changes of texture between the base material(BM) and the FZ were detected. The {0002} basal plane in the BM was largely parallel to the sheet rolling plane, whereas the c-axis of the crystal lattice in the FZ inclined approximately 25° with respect to the welding direction. The maximum pole density increased from 9.45 in the BM to 12.9 in the FZ. The microhardness distribution, tensile properties, and fracture features of the AZ31 auto-welded joints were also investigated.展开更多
A two-dimensional axisymmetric mathematical model of weld pool of pulsed TIG welding was established. Numerical simulation for weld pool of pulsed TIG welding was done using FLUENT software by selecting the appropriat...A two-dimensional axisymmetric mathematical model of weld pool of pulsed TIG welding was established. Numerical simulation for weld pool of pulsed TIG welding was done using FLUENT software by selecting the appropriate boundary conditions and strongly coupled control equations. The distributions of temperature field and flow field of weld pool under the periodic change of welding current were obtained. According to the maximum temperature of upper and lower surface of workpiece and depth and width of weld pool, the distributions of temperature field and flow field under different pulsed frequencies and current duty cycles were obtained and periodic variation was analyzed under pulsed current. The analysis results show that with the increase of pulsed frequency, weld pool width increases slightly while depth decreases slightly, and with the increase of current duty cycle, the width and depth of weld pool both increase significantly, and the depth increases greatly.展开更多
The effects of preheat treatments on the microstructures and mechanical properties of tungsten inert gas (TIG)-welded AZ61 magnesium alloy joints were studied by microstructural observations, microhardness tests and...The effects of preheat treatments on the microstructures and mechanical properties of tungsten inert gas (TIG)-welded AZ61 magnesium alloy joints were studied by microstructural observations, microhardness tests and tensile tests. The results showed that the vol- ume fraction of the lamellar β-Mg17(Al,Zn)12 intermetallic compound of in fusion zone (FZ) increased from 15% to 66% with an increase in preheat temperature. Moreover, the microhardness of the FZ and the ultimate tensile strength of the welded joints reached their maximum values when the preheat temperature was 300℃ because more lamellar β-Mg17(Al,Zn)12 intermetallic compounds were distributed at the α-Mg grain boundaries and no cracks and pores formed in the FZ of the welded joint.展开更多
A new twin-tungsten TIG (T-TIG) welding method was studied. This method differs from the conventional TIG method, it places two electrodes insulated from each other in the same welding torch, and a coupling arc is g...A new twin-tungsten TIG (T-TIG) welding method was studied. This method differs from the conventional TIG method, it places two electrodes insulated from each other in the same welding torch, and a coupling arc is generated from the two electrodes. The coupling arc pressure was measured and preliminary welding experiment was made. The results show that the coupling arc can keep arc pressure at a low level compared with conventional TIG arc, and welding can be achieved under higher current and high travel speed with sound appearance of weld. Therefore, this new method can applied widely in high effwiency welding.展开更多
The mechanism of penetration depth increased by activating flux in activating tungsten inert gas(A-TIG)weldingwas studied by measuring the distribution of trace element Bi in the weld and monitoring the change of arc ...The mechanism of penetration depth increased by activating flux in activating tungsten inert gas(A-TIG)weldingwas studied by measuring the distribution of trace element Bi in the weld and monitoring the change of arc voltageduring A-TIG welding of stainless steel 0Crl8Ni9 with fluxes SiO_(2)and TiO_(2).The results show that the mechanismof penetration depth in A-TIG welding depends on the sort of flux used.The weld pool convection after coating theflux SiO_(2)and flux TiO_(2)is changed inversely compared with convectional TIG welding without flux.The arc voltageis increased by flux SiO_(2)whilst flux TiO_(2)does not have effect on the arc voltage.The reason of penetration depthincrease for SiO_(2)is due to the constriction of arc plasma and the change of surface tension gradient.The increaseof weld penetration depth with TiO_(2)only ascribes to the change of surface tension gradient.展开更多
基金Funded by the Center of Excellence in Metals and Materials Engineering(CEMME),Faculty of Engineering,Prince of Songkla UniversitySupported by the National Science,Research and Innovation Fund(NSRF)and Prince of Songkla University(No.ENG6505079S)。
文摘Repair welding of AA 6082-T6 joints was carried out using ER 4043 filler through the TIG welding process with or without pulsed current.Microstructure and mechanical characteristics of the joints before and after repairing were investigated by examining macrostructure,microstructure,and distributions of porosity in the weld metal(WM),and by hardness,tensile,and bending tests.We observed that the welding current,phase transformations in heat-affected zone(HAZ)and porosity introduced in the WM during welding influence on its mechanical properties in sequence.The experimental results showed that the bead width and penetration as well as size of pores in the joints were mainly influenced by the welding currents.The sound joints were obtained at a welding current of 140 A with or without pulsed current when welding speed and gas flow rate were set at 20 cm·min-1 and 15 L·min-1,respectively.Among them,the decrease in mechanical properties of repair weld(RW)was directly related to the phase transformations in the over-ageing zone due to the double welding thermal cycles and elevated distribution of porosity in the WM.In addition,it was observed that the comparatively smaller grain size and lower porosity in WM of the RW produced by pulsed TIG welding gave a positive effect on its mechanical properties.
基金Project(2012ZX04010-081)supported by the National High-tech Research and Development Program of ChinaProject(CDJZR12110072)supported by Fundamental Research Funds for Central Universities of China
文摘A device for superimposing vibration on workpiece in both horizontal and vertical directions during tungsten-arc inert gas (TIG) welding was developed, with maximum power output of 2 kW at frequency of 15 kHz. AZ31 sheets with thickness of I and 3 mm were used in the vibratory welding. Microstructures along with the mechanical properties of the weld joints under different vibrating conditions (vibration direction, vibration amplitude and groove angle) were examined. It is observed that the grain size in welding zone decreases remarkably with the application of vibration, while the amount of second phase β-Mg_17Al_12 within the zone decreases slightly; meanwhile, microhardness of the weld joints, macroscopic tensile strength and elongation of the weldment increase. Vibration, especially the one along vertical direction, has more impact on the performance of the thick weldments. Influence of vibration on mierostructure and mechanical properties of weldments is affected by wave energy transferring in the melt and depends on the processing and geometric parameters including amplitude and direction of vibration, thickness, and groove angles.
文摘采用TIG(Tungsten inert gas welding,TIG)焊对FeCrAl合金管同质材料进行焊接,通过扫描电子显微镜、透射电子显微镜及能谱仪等手段研究了焊后接头的显微组织特征、焊后接头不同区域氧化物颗粒的分布情况及焊接接头的力学性能。FeCrAl合金TIG焊通过填充等成分的FeCrAl合金丝材进行焊接,焊后焊接接头主要由焊缝区、热影响区及母材组成。其中焊缝区为粗大的铁素体组织,热影响区为细小的等轴晶组织。焊缝区的Y_(2)O_(3)氧化物颗粒发生了明显粗化并与基体反应生成复合氧化物Y_(3)Al_(5)O_(12)。TIG焊焊接FeCrAl合金管热处理后,焊接接头最大抗拉强度值为530 MPa,约为母材强度的80.8%,可以实现大口径、大壁厚的FeCrAl合金管材的对接接头的力学性能要求。
基金Project (51001034) supported by the National Natural Science Foundation of ChinaProject (208181) supported by the Key Project of Chinese Ministry of Education+1 种基金Projects (2008AA4CH044, 2009AA1AG065, 2010AA4BE031) supported by the Key Project of Science and Technology of Harbin City, ChinaProject (HEUCF101001) supported by the Fundamental Research Funds for the Central Universities, China
文摘Tungsten inert gas weld was carried out on super-light magnesium-lithium alloy plates with a thickness of 2 mm, using argon gas as a protecting atmosphere. The microstructure and mechanical properties of the welded joints were investigated. The results indicate that the microstructure in the fusion zone is fine, and the microstructure in the heat-affected zone is coarser than the parent metal. The tensile strength of the welded joint is about 84% that of the parent metal. The fracture occurs in a mixed type of toughness and brittleness in the heat-affected zone. During the welding process, aluminum and cerium are enriched at grain boundaries in the fusion zone.
文摘The ultrasonic assisted tungsten inert gas (U-TIG) welding is a newly developed arc welding method, which is aimed at improving the weld quality and efficiency. TIG welding and U-TIG welding of 2014 aluminum alloy with 5 mm thickness were experimentally carried out in this paper. The microstructure and porosity of welded joints were analyzed. Compared with conventional TIG welding, the columnar crystals are changed into equiaxed crystals at the centre of weld zone and the grain of fusion zone in U-TIG welding is refined and equiaxed. The porosities of joint decrease after the ultrasonic was applied on the arc. The mechanism of crystal grain refinement is discussed in this paper and the reasons of porosity decrease in U-TIG welded joint may be due to the effect of acoustic streaming and cavitation, which need further research.
基金supported by National Natural Science Foundation of China(Grant No.51265029)
文摘This paper deals with a novel dual shield TIG welding method named gas pool coupled activating TIG( GPCA-TIG)welding. The welding method divides the shielding gas into two layers. Inert gas such as Ar is adopted as the inner layer gas to protect the tungsten electrode and the molten pool metal. Pure O_2,N_2 or mixture of them are used as the outer layer gas to increase the weld penetration and improve the low temperature toughness of weld metal. Through analyzing the interaction between outer gas and arc and the distributions and existing forms of oxygen and nitrogen elements,the transfer behaviors of nitrogen and oxygen from arc to pool were investigated. The results show that,the interaction between the outer gas and arc plasma makes the arc slightly constrict. The incoming oxygen enriches on the molten pool surface and exists in the form of iron oxide,chromium oxide,manganese oxide and silicon oxygen compounds. The incoming nitrogen evenly distributes in the molten pool and exists in the form of nitrogen atom.
基金China Postdoctoral Science Foundation (No 20080430129)
文摘Three-dimensional finite element model was established to simulate temperature fields of T-joint titanium sheets during TIG welding with finite element method (FEM) software. Temperature dependent material properties and the effect of latent heat were considered. A technique of element birth and death was used to simulate the process of welded metal filling. Dynamic variation process of temperature fields during T1G welding was achieved. The simulated results agreed well with the measured results.
文摘In order to realize automatic control of the width of weld pool, a visual sensor system for the width of weld pool detection is developed. By initiative arc light, the image of copper plate weld pool is taken back of the torch through the process of weakening and filtering arc light. In order to decrease the time of processing video signals, analog circuit is applied in the processing where video signals is magnified, trimmed and processed into binary on the datum of dynamic average value, therefore the waveform of video signals of weld pool is obtained. The method that is used for detecting the width of weld pool is established. Results show that the vision sensing method for real-time detecting weld pool width to copper-clad aluminum wire TIG welding is feasible. The response cycle of this system is no more than 50 ms, and the testing precision is less than 0. 1 mm.
文摘Methods of arc length control and visual image based weld detection for precision pulse TIG welding were investigated. With a particular all hardware circuit, arc voltage during peak current stage is sampled and integrated to indicate arc length, deviation of arc length and adjusting parameters are calculated and output to drive a step motor directly. According to the features of welding image grabbed with CCD camera, a special algorithm was developed to detect the central line of weld fast and accurately. Then an application system were established, whose static arc length error is ±0.1 mm with 20 A average current and 1 mm given arc length, static detection precision of weld is 0.01 mm , processing time of each image is less than 120 ms . Precision pulse TIG welding of some given thin stainless steel components with complicated curved surface was successfully realized.
基金supported by the National Key Research and Development Plan of China(Grant Nos.2016YFB0701200 and 2016YFB0301105)the Natural Science Foundation of Shandong Province,China(Grant Nos.ZR2015EQ019,BS2015CL016,and ZR2015YL007)the Youth Foundation of Shandong Academy of Sciences,China(Grant No.2016QN015)
文摘The automatic tungsten-inert gas welding(ATIGW) of AZ31 Mg alloys was performed using a six-axis robot. The evolution of the microstructure and texture of the AZ31 auto-welded joints was studied by optical microscopy, scanning electron microscopy, energy-dispersive X-ray spectroscopy, and electron backscatter diffraction. The ATIGW process resulted in coarse recrystallized grains in the heat affected zone(HAZ) and epitaxial growth of columnar grains in the fusion zone(FZ). Substantial changes of texture between the base material(BM) and the FZ were detected. The {0002} basal plane in the BM was largely parallel to the sheet rolling plane, whereas the c-axis of the crystal lattice in the FZ inclined approximately 25° with respect to the welding direction. The maximum pole density increased from 9.45 in the BM to 12.9 in the FZ. The microhardness distribution, tensile properties, and fracture features of the AZ31 auto-welded joints were also investigated.
基金This work was financially supported by National Natural Science Foundation of China No. 51205179.
文摘A two-dimensional axisymmetric mathematical model of weld pool of pulsed TIG welding was established. Numerical simulation for weld pool of pulsed TIG welding was done using FLUENT software by selecting the appropriate boundary conditions and strongly coupled control equations. The distributions of temperature field and flow field of weld pool under the periodic change of welding current were obtained. According to the maximum temperature of upper and lower surface of workpiece and depth and width of weld pool, the distributions of temperature field and flow field under different pulsed frequencies and current duty cycles were obtained and periodic variation was analyzed under pulsed current. The analysis results show that with the increase of pulsed frequency, weld pool width increases slightly while depth decreases slightly, and with the increase of current duty cycle, the width and depth of weld pool both increase significantly, and the depth increases greatly.
基金supported by the Key Scientific and Technological Project of Chongqing (No.CSTC, 2009AC4046)Natural Science Foundation Project of CQ CSTC (No. CSTC, 2010BB4039) Fundamental Research Funds for the Central Universities of China (Nos.CDJZR10130010 and CDJXS10131155)
文摘The effects of preheat treatments on the microstructures and mechanical properties of tungsten inert gas (TIG)-welded AZ61 magnesium alloy joints were studied by microstructural observations, microhardness tests and tensile tests. The results showed that the vol- ume fraction of the lamellar β-Mg17(Al,Zn)12 intermetallic compound of in fusion zone (FZ) increased from 15% to 66% with an increase in preheat temperature. Moreover, the microhardness of the FZ and the ultimate tensile strength of the welded joints reached their maximum values when the preheat temperature was 300℃ because more lamellar β-Mg17(Al,Zn)12 intermetallic compounds were distributed at the α-Mg grain boundaries and no cracks and pores formed in the FZ of the welded joint.
文摘A new twin-tungsten TIG (T-TIG) welding method was studied. This method differs from the conventional TIG method, it places two electrodes insulated from each other in the same welding torch, and a coupling arc is generated from the two electrodes. The coupling arc pressure was measured and preliminary welding experiment was made. The results show that the coupling arc can keep arc pressure at a low level compared with conventional TIG arc, and welding can be achieved under higher current and high travel speed with sound appearance of weld. Therefore, this new method can applied widely in high effwiency welding.
基金This work was supported by the National High Technology Research and Developrment Program of China under grant Nc.200AA331160the Scientifc Research Foundation of Harbin Institute of Technology under grant No.H.IT.2001.20.
文摘The mechanism of penetration depth increased by activating flux in activating tungsten inert gas(A-TIG)weldingwas studied by measuring the distribution of trace element Bi in the weld and monitoring the change of arc voltageduring A-TIG welding of stainless steel 0Crl8Ni9 with fluxes SiO_(2)and TiO_(2).The results show that the mechanismof penetration depth in A-TIG welding depends on the sort of flux used.The weld pool convection after coating theflux SiO_(2)and flux TiO_(2)is changed inversely compared with convectional TIG welding without flux.The arc voltageis increased by flux SiO_(2)whilst flux TiO_(2)does not have effect on the arc voltage.The reason of penetration depthincrease for SiO_(2)is due to the constriction of arc plasma and the change of surface tension gradient.The increaseof weld penetration depth with TiO_(2)only ascribes to the change of surface tension gradient.