Size effect on longitudinal MOE of microtomed wood sections and relevant theoretical explanation 被引量:2
1
作者 YU Yan JIANG Ze-hui TIAN Gen-lin 《Forestry Studies in China》 CAS 2009年第4期243-248,共6页
It has been repeatedly observed that the mechanical properties of microtomed wood sections are significantly lower than those of samples of normal size, but few investigations have been conducted to deal with this top... It has been repeatedly observed that the mechanical properties of microtomed wood sections are significantly lower than those of samples of normal size, but few investigations have been conducted to deal with this topic, especially based on theoretical approaches. We measured the longitudinal MOE of Chinese fir on microtomed sections ranging in thickness from 70 to 200 μm and compared these with the values of samples of normal size. The results indicate that the MOE of microtomed wood sections increases with thickness from 70 to 200 μm, but is significantly less than that of normal samples. A size effect coefficient of 2.63 is inferred based on statistical data for samples of normal size and 200 μm thick microtomed sections. Finally, an explanation based on a complete shear restraint model of cell walls and a single fiber multi-ply model is proposed for the size effect on stiffness of microtomed wood sections. 展开更多
关键词 a complete shear restraint model microtomed wood sections a single fiber multi-ply model size effect
下载PDF
纤维粒径对荔枝修枝木/高密度聚乙烯复合材料性能的影响
2
作者 陈世桓 周桥芳 +3 位作者 王先菊 云虹 胡传双 涂登云 《木材科学与技术》 北大核心 2023年第3期35-43,共9页
为了解决荔枝修枝木的利用问题,以荔枝修枝木纤维和高密度聚乙烯为主要原料,采用挤出成型的方法制备荔枝修枝木/HDPE复合材料(LWPC)。采用热重法测定荔枝木的热稳定性,利用体式显微镜观察荔枝木纤维形态,分析荔枝木纤维粒径对LWPC性能... 为了解决荔枝修枝木的利用问题,以荔枝修枝木纤维和高密度聚乙烯为主要原料,采用挤出成型的方法制备荔枝修枝木/HDPE复合材料(LWPC)。采用热重法测定荔枝木的热稳定性,利用体式显微镜观察荔枝木纤维形态,分析荔枝木纤维粒径对LWPC性能的影响。结果表明:荔枝木纤维初始降解温度为255℃;随着荔枝木纤维粒径的减小,其长径比先增大后逐渐减小。在动态流变测试中,随着荔枝木纤维粒径的减小,LWPC熔体的平衡转矩和平衡剪切热先降低后升高,储能模量、损耗模量和复数黏度增加。在动态热机械测试中,随着荔枝木纤维粒径的减小,LWPC的储能模量、损耗模量逐渐增大。LWPC的密度、吸水率、弯曲及拉伸性能呈现增大趋势,吸水厚度膨胀率则呈减小趋势。综合考虑LWPC的加工流变性能和物理力学性能,宜选用粒径<300μm的荔枝木纤维,制得LWPC的弯曲强度、弯曲模量最高分别为31.11 MPa、2.91 GPa,达到GB/T 24137—2009《木塑装饰板》的要求。 展开更多
关键词 荔枝木 木纤维粒径 木塑复合材料 力学性能 流变性能
下载PDF
纤维粒径对木塑复合材料抗老化性能的影响 被引量:14
3
作者 王伟宏 王晶晶 +2 位作者 黄海兵 隋淑娟 王清文 《高分子材料科学与工程》 EI CAS CSCD 北大核心 2014年第5期92-97,共6页
研究了不同粒径木纤维(120 mesh^80 mesh、80 mesh^40 mesh、40 mesh^20 mesh、20 mesh^10 mesh)增强的高密度聚乙烯基复合材料的抗紫外加速老化性能。研究表明,含较大粒径木纤维的木塑复合材料抗弯曲性能最好,但冲击强度最差。经过200... 研究了不同粒径木纤维(120 mesh^80 mesh、80 mesh^40 mesh、40 mesh^20 mesh、20 mesh^10 mesh)增强的高密度聚乙烯基复合材料的抗紫外加速老化性能。研究表明,含较大粒径木纤维的木塑复合材料抗弯曲性能最好,但冲击强度最差。经过2000 h的紫外加速老化后,复合材料的抗弯强度和弹性模量损失最大分别可达18%和34%,但抗冲击性能有所增强,其中20 mesh^10 mesh木纤维复合材料的冲击强度变为最大值。扫描电子显微镜观察到纤维粒径大的复合材料老化后破坏较严重,傅里叶变换红外光谱分析认为表面有氧化发生,但凝露时水分冲刷影响了表面氧化探测的准确性。 展开更多
关键词 木纤维粒径 高密度聚乙烯 复合材料 紫外老化 性能分析
下载PDF
JN型微米木纤维减震器
4
作者 马岩 张亚新 +2 位作者 袁旭 战丽 杨春梅 《林业科学》 EI CAS CSCD 北大核心 2015年第1期112-118,共7页
【目的】利用微米木纤维为原材料代替难以降解的橡胶和塑料,制作出适用于机械设备或汽车减震装置的JN型木纤维减震器,研究JN型木纤维减震器的选材、加工工艺及数学建模方法,为减震器数控加工机床和数控系统的研制与开发提供理论依据。... 【目的】利用微米木纤维为原材料代替难以降解的橡胶和塑料,制作出适用于机械设备或汽车减震装置的JN型木纤维减震器,研究JN型木纤维减震器的选材、加工工艺及数学建模方法,为减震器数控加工机床和数控系统的研制与开发提供理论依据。【方法】以密度为0.439 g·cm-3、含水率为12%~15%、平均厚度可达到52μm的红松微米木纤维为基材,利用冷硫化和复合材组构理论,采用热压模具定型方法制作出JN型微米木纤维减震器样品,测量样品的质量、体积并观察样品浸泡在水中24 h后的外形状态。在基本假设的基础上,用包络法和规则几何体建模法建立JN型微米木纤维减震器的数学模型,并利用Matlab软件对JN型微米木纤维减震器进行仿真分析。【结果】JN型微米木纤维减震器样品的密度在0.91~1.36 g·cm-3之间,质量在1.4~2.0 kg之间,在水中浸泡24 h不会变形。仿真分析结果证明JN型微米木纤维减震器数学模型具有一定的通用性和准确性。【结论】按规定的加工工艺制备的JN型微米木纤维减震器样品符合密度、弹性要求,并且具有抗水性;JN型木纤维减震器的建模由底座和规则梯形台构成,模型参数具有通用性,直接将底座和规则梯形面相关尺寸参数输入模型方程,可获得JN型木纤维减震器的不同加工尺寸;为保证JN型木纤维减震器的实用尺寸和外观,降低生产成本,整个模压加工过程必须在一套模具上完成。 展开更多
关键词 微米木纤维 木橡胶 减震器 数学建模
下载PDF
Effect of Wood Variables on the Properties of Wood Fiber-Polypropylene Composites 被引量:1
5
作者 Kouichi SETOYAMA 《Chinese Forestry Science and Technology》 2002年第4期47-54,共8页
The effect of wood species (Chinese fir and Poplar), wood fiber content (10%, 25%, 40%) and wood fiber sizes (16 to 32 mesh, 32-65 mesh, above 65 mesh) on the properties of the wood fiber-Polypropylene composites were... The effect of wood species (Chinese fir and Poplar), wood fiber content (10%, 25%, 40%) and wood fiber sizes (16 to 32 mesh, 32-65 mesh, above 65 mesh) on the properties of the wood fiber-Polypropylene composites were studied in this paper. The results indicate that the effect of wood fiber content and size in composite were more important than that of chosen wood species. Compared with polypropylene without wood fiber, the flexural strength of the composites increased when adding wood fiber into polypr... 展开更多
关键词 wood fiber/polypropylene composite wood fiber content wood fiber size dynamic mechanical properties
原文传递
木纤维尺寸对聚乳酸木纤维复合材料性能的影响 被引量:8
6
作者 吴蕴忱 刘珊杉 刘巍岩 《林业科技》 2017年第4期23-26,共4页
采用3种长径比的杨木纤维作为原料,与聚乳酸复合制成木纤维/聚乳酸复合材料。通过对比3种复合材料的静曲强度、弹性模量、拉伸强度和冲击强度发现,含有中等尺寸木纤维复合材料的综合物理力学性能较高,而含有较小尺寸木纤维复合材料的拉... 采用3种长径比的杨木纤维作为原料,与聚乳酸复合制成木纤维/聚乳酸复合材料。通过对比3种复合材料的静曲强度、弹性模量、拉伸强度和冲击强度发现,含有中等尺寸木纤维复合材料的综合物理力学性能较高,而含有较小尺寸木纤维复合材料的拉伸强度较高,含有较大尺寸木纤维的样品综合性能较差。研究结果表明,纤维的分散性、体系的均匀性以及界面结合度对复合材料的各项物理力学性能影响最大,而木纤维的尺寸很大程度上决定了其分散性和界面结合面积,因此,添加适当尺寸的木材纤维能够对木纤维/聚乳酸复合材料的力学性能产生相应的增强效果。 展开更多
关键词 木材纤维 聚乳酸 复合材料 力学性能 纤维尺寸
下载PDF
杨木纤维尺寸对环氧树脂复合材料力学性能的影响 被引量:1
7
作者 马红亮 陈健 +3 位作者 焦健 邓拥军 孔振武 房桂干 《林产化学与工业》 EI CAS CSCD 北大核心 2020年第2期104-108,共5页
由木材剩余物杨木枝桠材为原料,制得杨木纤维的化学机械浆后,经直接烘干和溶剂置换两种不同的后续处理方法得到不同尺寸杨木纤维(PWF),再与环氧树脂E51经热压成型制备PWF增强环氧树脂(PWF/E51)复合材料。通过PWF微观形貌与尺寸分析,结合... 由木材剩余物杨木枝桠材为原料,制得杨木纤维的化学机械浆后,经直接烘干和溶剂置换两种不同的后续处理方法得到不同尺寸杨木纤维(PWF),再与环氧树脂E51经热压成型制备PWF增强环氧树脂(PWF/E51)复合材料。通过PWF微观形貌与尺寸分析,结合PWF/E51复合材料冲击断面微观形貌分析,探讨了PWF尺寸对PWF/E51复合材料力学性能的影响。研究结果表明:PWF尺寸对增强环氧树脂复合材料力学性能有较大影响,随PWF长径比增大,复合材料的冲击强度和弯曲强度均先增大后减小,其中溶剂置换处理的PWF/E51复合材料(长径比值14.8)力学强度最佳,冲击强度7.1 kJ/m2,弯曲强度68.2 MPa。此外,经溶剂置换处理的PWF/E51复合材料的力学强度较直接烘干处理有所提高。 展开更多
关键词 杨木纤维 纤维尺寸 环氧树脂 复合材料 力学性能
下载PDF
木粉对PVC发泡木塑复合材料性能的影响 被引量:2
8
作者 刘建中 李先红 +7 位作者 张洋 李影 庞磊 刘涛 葛静瑞 庾文学 周永胜 熊建平 《广州化工》 CAS 2014年第9期80-83,共4页
采用PVC树脂和木粉加入发泡剂制得PVC/木粉发泡复合材料。本文对木粉进行了热重分析,考察木粉粒径及含量对PVC/木塑发泡材料性能的影响,考察了木粉含量对发泡、熔融指数、转矩加工流变性以及耐候性的影响。结果表明:TG分析表明PVC/木塑... 采用PVC树脂和木粉加入发泡剂制得PVC/木粉发泡复合材料。本文对木粉进行了热重分析,考察木粉粒径及含量对PVC/木塑发泡材料性能的影响,考察了木粉含量对发泡、熔融指数、转矩加工流变性以及耐候性的影响。结果表明:TG分析表明PVC/木塑复合材料加工的最佳温度200℃左右。随着木粉粒径的减小,PVC/木粉复合材料的冲击强度和弯曲强度出现先上升后下降的趋势,100目木粉,力学性能最好。随着木粉用量的增加,体系的拉伸强度、冲击强度和弯曲强度均呈降低的趋势,材料的发泡效果变差,流动性、稳定性、耐候性变差,因此PVC木塑复合材料应该控制其木粉含量。 展开更多
关键词 木粉 PVC 木塑复合材料 力学性能 粒径 熔体流动速率
下载PDF
碳纤维增强木粉/聚乙烯复合材料的制备及其力学性能 被引量:7
9
作者 杜凤 王伟宏 《南京林业大学学报(自然科学版)》 CAS CSCD 北大核心 2015年第2期132-136,共5页
将短切碳纤维(SCF)与木粉(WF)、高密度聚乙烯(HDPE)塑料和其他添加剂共混、熔融复合后,用模压成型方法制备了短切碳纤维增强木塑(SCF/WF/HDPE)复合材料;将碳布放置于木塑板上下表面,经模压成型制备碳纤维布增强木塑(CFC/WF/HDPE)复合材... 将短切碳纤维(SCF)与木粉(WF)、高密度聚乙烯(HDPE)塑料和其他添加剂共混、熔融复合后,用模压成型方法制备了短切碳纤维增强木塑(SCF/WF/HDPE)复合材料;将碳布放置于木塑板上下表面,经模压成型制备碳纤维布增强木塑(CFC/WF/HDPE)复合材料。研究了碳纤维用量对碳纤维增强WF/HDPE复合材力学性能的影响,并利用扫描电镜(SEM)和红外光谱(FTIR)对碳纤维进行表征。结果表明:与纯WF/HDPE复合材相比,碳纤维加入量为10%时,复合材料的力学强度提高幅度最大,拉伸强度和弯曲强度分别提高了8.4%和10.6%;当碳纤维加入量为6%时,复合材料的韧性提高幅度最大,断裂伸长率提高了25.9%,冲击强度提高了24.4%。使用丙酮清洗掉碳纤维表面的上浆剂后,其增强效果比未经过处理的碳纤维略有下降。与短切碳纤维相比,碳布的增强效果更好,与短切碳纤维增强木塑(SCF/WF/HDPE)复合材料相比,碳布平铺在木塑板表面的结构拉伸性能可提高62%,断裂伸长率提高148%,弯曲强度提高71%,冲击强度提高313%。 展开更多
关键词 木塑复合材料 碳纤维 力学性能 上浆剂
原文传递
草浆中性造纸系统的留着与滤水特性
10
作者 朱勇强 《上海造纸》 2004年第3期41-43,共3页
迄今为止,草浆仍然是国内造纸的主要原料,而草浆中因含有大量的杂细胞,其特性与木浆截然不同。本文系统地介绍了采用松香中性施胶的草浆造纸系统的留着与滤水特性,主要从以下几个方面进行了讨论:(1)草浆的留着特点;(2)配套助剂R100对纸... 迄今为止,草浆仍然是国内造纸的主要原料,而草浆中因含有大量的杂细胞,其特性与木浆截然不同。本文系统地介绍了采用松香中性施胶的草浆造纸系统的留着与滤水特性,主要从以下几个方面进行了讨论:(1)草浆的留着特点;(2)配套助剂R100对纸料留着和滤水性能的影响;(3)改性淀粉对留着和滤水性能的影响;(4)配套助剂RG03对留着和滤水性能的影响;(5)添加顺序对留着和滤水性能的影响;(6)流体剪切力和助留剂与细小组分的留着。 展开更多
关键词 草浆 造纸 留着 滤水特性 湿部化学 流体剪切力 松香中性施胶