Evolution of inner wall wrinkle defects in the sinking zone of a thick-walled steel tube during radial forging
1
作者 Yu-Zhao Yang Cheng Xu Li-Xia Fan 《Advances in Manufacturing》 SCIE EI CAS CSCD 2024年第2期396-408,共13页
An axial wrinkle defect was observed in the inner wall of the sinking zone of a thick-wall steel tube processed by cold radial forging.Wrinkles can evolve into fissures.The present study focuses on the evolution of wr... An axial wrinkle defect was observed in the inner wall of the sinking zone of a thick-wall steel tube processed by cold radial forging.Wrinkles can evolve into fissures.The present study focuses on the evolution of wrinkles and the effects of process parameters on them using a three-dimensional radial forging process finite element model,radial forging experiments,and surface morphology observations.The results indicated that the vertical section angle of the hammer die and the size of the tube blank significantly affect the evolution of wrinkles.The height-to-width ratioλwas introduced to describe the morphology of wrinkles.It had an approximately linear relationship with the radius reduction in the sinking zone.There was a linear correlation between the growth slope ofλand the axial to circumferential strain ratio|εr/εθ|,which can predict theλunder few process parameters.For the 30SiMn2MoVA steel,at the junction of the forging and sinking zones,the threshold ofλof the wrinkle that can evolve into a fissure is approximately 1.123. 展开更多
关键词 Radial forging Inner wall Wrinkle defects EVOLUTION Sinking zone
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部