The total ribbon voltage of as-quenched and annealed Fe96-xZr_xB_4 (x=7 or 10) ribbons has been measured as a function of applied dc field and drive current frequency. The experimental results show that both samples e...The total ribbon voltage of as-quenched and annealed Fe96-xZr_xB_4 (x=7 or 10) ribbons has been measured as a function of applied dc field and drive current frequency. The experimental results show that both samples exist the optimum annealing temperature and optimum frequency at which the relative change in ribbon voltage is strongest, and the sensitivity of the magnetic response of the annealed Fe_89Zr_7B_4 ribbon is two order of magnitude larger than that of the annealed Fe_86Zr_10 B4 ribbon. The effect of magnetic properties and structural characteristics on giant magneto-impedance was discussed.展开更多
文摘The total ribbon voltage of as-quenched and annealed Fe96-xZr_xB_4 (x=7 or 10) ribbons has been measured as a function of applied dc field and drive current frequency. The experimental results show that both samples exist the optimum annealing temperature and optimum frequency at which the relative change in ribbon voltage is strongest, and the sensitivity of the magnetic response of the annealed Fe_89Zr_7B_4 ribbon is two order of magnitude larger than that of the annealed Fe_86Zr_10 B4 ribbon. The effect of magnetic properties and structural characteristics on giant magneto-impedance was discussed.