Preparation of ZrB_(2)-ZrO_(2)-SiC Composite Powder by Carbothermal Reduction from Zircon
1
作者 TIAN Xuekun ZHOU Chaojie +4 位作者 ZHANG Lei ZHAO Fei JIA Quanli LIU Xinhong ZHONG Xiangchong 《China's Refractories》 CAS 2023年第1期25-29,共5页
Using zircon,boric acid and carbon black as starting materials,ZrB_(2)-ZrO_(2)-SiC composite powder was synthesized by calcining at 1500℃in flowing argon atmosphere.The effects of the soaking time(3,6 and 9 h)and the... Using zircon,boric acid and carbon black as starting materials,ZrB_(2)-ZrO_(2)-SiC composite powder was synthesized by calcining at 1500℃in flowing argon atmosphere.The effects of the soaking time(3,6 and 9 h)and the addition of additive AlF_(3)(0,0.5%,1.0%,1.5%,2.0%and 2.5%,by mass)on the phase composition and the microstructure of the synthesized products were investigated.The results show that:(1)ZrB_(2)-ZrO_(2)-SiC composite powder can be synthesized by carbothermal reduction at 1500℃in flowing argon atmosphere;ZrB_(2) and ZrO_(2) are granular-like,and SiC crystals are fiberous;(2)with the soaking time increasing,the amount of ZrB_(2) increases,the amounts of m-ZrO_(2) and SiC decrease,and the total amount of non-oxides ZrB_(2),SiC and ZrC gradually increases;the optimal soaking time is 3 h;(3)compared with the sample without AlF_(3),the sample with 0.5% AlF_(3) has decreased m-ZrO_(2)amount,noticeably increased ZrB_(2) amount but decreased SiC amount;however,when the addition of AlF_(3) increases from 0.5%to 2.5%,the m-ZrO_(2) amount increases,the ZrB_(2)amount decreases,and the SiC amount changes slightly;the optimum AlF_(3)addition is 0.5%. 展开更多
关键词 ZIRCON carbothermal reduction zirconium diboride-zirconia-silicon carbide composite powder
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部