Supported multi-metal catalyst was prepared by impregnation.A variety of factors such as reaction temperature, feedstock ratio, alkali concentration, catalyst concentration and antipolymerizer concentration were syste...Supported multi-metal catalyst was prepared by impregnation.A variety of factors such as reaction temperature, feedstock ratio, alkali concentration, catalyst concentration and antipolymerizer concentration were systematically investigated in terms of their effects on the oxidative esterification reaction for methyl methacrylate production from methacrolein.The experimental results showed that under the condition of temperature 333 K,methanol/methacrolein ratio 97∶1(molar ratio),NaOH concentration 0.001 g·ml^-1 and catalyst concentration 0.02 g·ml^-1, methacrolein conversion and methyl methacrylate selectivity were about 100% and 71.4% respectively, after 30 min reaction.展开更多
文摘Supported multi-metal catalyst was prepared by impregnation.A variety of factors such as reaction temperature, feedstock ratio, alkali concentration, catalyst concentration and antipolymerizer concentration were systematically investigated in terms of their effects on the oxidative esterification reaction for methyl methacrylate production from methacrolein.The experimental results showed that under the condition of temperature 333 K,methanol/methacrolein ratio 97∶1(molar ratio),NaOH concentration 0.001 g·ml^-1 and catalyst concentration 0.02 g·ml^-1, methacrolein conversion and methyl methacrylate selectivity were about 100% and 71.4% respectively, after 30 min reaction.