In situ thickness dependent photoluminescence (PL) measurements of tris(8-hydroxyquinoline) aluminum(Alq3) film were performed. At the beginning of Alq3 deposition on the glass substrate, the Alq3 emission showe...In situ thickness dependent photoluminescence (PL) measurements of tris(8-hydroxyquinoline) aluminum(Alq3) film were performed. At the beginning of Alq3 deposition on the glass substrate, the Alq3 emission showed a sharp red-shift. Further deposition of Alq3 resulted slight red-shift, and finally tended to saturated value. The total red-shift of about 12 nm was observed for the Alq3 film thickness range from 2 to 500 nm.This red-shift was attributed to the change from the 2D to 3D exciton state with increasing Alq3 film thickness. Meanwhile, the PL intensity of Alq3 emission increased continuously, and showed a rate change at the initial deposition of Alq3 due to non-rediative decay of excitons arised from the interaction between excitons and the substrate, and finally tended to saturation with the Alq3 thickness.展开更多
基金This work is supported by the National Natural Science Foundation of China (No. 10274072, 20240430654)the Specialized Research Fund for the Doctoral Program of Higher Education of China (No. 20030335017).
文摘In situ thickness dependent photoluminescence (PL) measurements of tris(8-hydroxyquinoline) aluminum(Alq3) film were performed. At the beginning of Alq3 deposition on the glass substrate, the Alq3 emission showed a sharp red-shift. Further deposition of Alq3 resulted slight red-shift, and finally tended to saturated value. The total red-shift of about 12 nm was observed for the Alq3 film thickness range from 2 to 500 nm.This red-shift was attributed to the change from the 2D to 3D exciton state with increasing Alq3 film thickness. Meanwhile, the PL intensity of Alq3 emission increased continuously, and showed a rate change at the initial deposition of Alq3 due to non-rediative decay of excitons arised from the interaction between excitons and the substrate, and finally tended to saturation with the Alq3 thickness.