A series of (Ag0.9Li0.1)(Nb1-yTay)O3 ceramic powders were prepared by an aque-chemical method. The optimized calcination temperature, time and crystal lattice were studied by TG-DTA, IR, XRD and TEM. The results show ...A series of (Ag0.9Li0.1)(Nb1-yTay)O3 ceramic powders were prepared by an aque-chemical method. The optimized calcination temperature, time and crystal lattice were studied by TG-DTA, IR, XRD and TEM. The results show that the optimized conditions were calcination of the precursor at 800 ℃ for 2 h. The ceramic powder thus prepared was rhombohedral with the average grain size of 48 nm.展开更多
文摘A series of (Ag0.9Li0.1)(Nb1-yTay)O3 ceramic powders were prepared by an aque-chemical method. The optimized calcination temperature, time and crystal lattice were studied by TG-DTA, IR, XRD and TEM. The results show that the optimized conditions were calcination of the precursor at 800 ℃ for 2 h. The ceramic powder thus prepared was rhombohedral with the average grain size of 48 nm.