Steel piles at the tidal zone can be seriously corroded. Common protective methods such as painting or coating with rubber or other protective materials, etc. cannot provide full protection when used as supplementary ...Steel piles at the tidal zone can be seriously corroded. Common protective methods such as painting or coating with rubber or other protective materials, etc. cannot provide full protection when used as supplementary protection because these traditional methods require strict pretreatment and sealing of the metallic surface from the corrosive mediums.and time for the protective coatings to solidify. This is very difficult under the severe action of waves and surges on the sea.With our oil-soluble DZ-2 tape, protection efficiency for hanging steel plates at the tidal and splash zones reaches to 82-99%. The protection efficiency of water soluble DZ tape at the tidal zone reaches to 92.9%. The DZ and DZ-2 tapes can rapidly reduce the original corrosion velocity to ten percent and one percent respectively as fully proved by the 500 hour rapid corrosion testing with indoor salt fog and by the relevant electrochemical parameters of instantaneous corrosion velocity,etc.DZ tape absorbs much OH- to cause a pH展开更多
文摘Steel piles at the tidal zone can be seriously corroded. Common protective methods such as painting or coating with rubber or other protective materials, etc. cannot provide full protection when used as supplementary protection because these traditional methods require strict pretreatment and sealing of the metallic surface from the corrosive mediums.and time for the protective coatings to solidify. This is very difficult under the severe action of waves and surges on the sea.With our oil-soluble DZ-2 tape, protection efficiency for hanging steel plates at the tidal and splash zones reaches to 82-99%. The protection efficiency of water soluble DZ tape at the tidal zone reaches to 92.9%. The DZ and DZ-2 tapes can rapidly reduce the original corrosion velocity to ten percent and one percent respectively as fully proved by the 500 hour rapid corrosion testing with indoor salt fog and by the relevant electrochemical parameters of instantaneous corrosion velocity,etc.DZ tape absorbs much OH- to cause a pH