ZSM-5 zeolite with a hexagonal cubic morphology was synthesized by a hydrothermal method using Triton X-100, a nonionic surfactant. The samples prepared with and without the surfactant were characterized by X-ray diff...ZSM-5 zeolite with a hexagonal cubic morphology was synthesized by a hydrothermal method using Triton X-100, a nonionic surfactant. The samples prepared with and without the surfactant were characterized by X-ray diffraction(XRD), Fourier transform infrared spectroscopy, N2 adsorption, high resolution transmission electron microscopy(TEM), high resolution scanning electron mi-croscopy, energy dispersive X-ray analysis, and NH3 temperature-programmed desorption. The XRD patterns confirmed the formation of a pure ZSM-5 crystalline phase without secondary phases. TEM images revealed that the hexagonal cubes were made of peanut-shaped nanoparticles with voids.The catalytic activity of the zeolite samples was evaluated using the selective oxidation of benzyl alcohol with tertiary-butyl hydrogen peroxide as the oxidant at 90 °C. The surfactant-assisted prep-aration yielded a zeolite that gave a higher conversion than the one prepared in the absence of the surfactant. The catalyst was retrieved and reused four times without significant loss in activity and selectivity.展开更多
Un-doped and Co-doped ZnO nanoparticles (NPs) with different weight ratios (0.5, 1.0, 1.5, and 2.0 wt% of Co) were synthesized by a facile and rapid microwave-assisted combustion method using urea as a fuel. The p...Un-doped and Co-doped ZnO nanoparticles (NPs) with different weight ratios (0.5, 1.0, 1.5, and 2.0 wt% of Co) were synthesized by a facile and rapid microwave-assisted combustion method using urea as a fuel. The prepared NPs were characterized by X-ray diffraction (XRD), high resolution scanning electron microscopy (HR-SEM), energy dispersive X-ray analysis (EDX), diffuse reflectance spectroscopy (DRS), photoluminescence (PL) spectroscopy and vibrating sample magnetometry (VSM). XRD patterns refined by the Rietveld method indicated that Co-doped ZnO had a single pure phase with wurtzite structure suggesting that Co^2+ ions would occupy Zn^2+ ionic sites within the ZnO crystal lattice. Interestingly, the morphology was found to convert substantially from grains to nanoparticles with close-packed periodic array of hexagonal-like shape and then into randomly distributed spherical NPs with the variation of Co-content. The optical band gap estimated using DRS was found to be red-shifted from 3.22 eV for the un-doped ZnO NPs then decrease up to 2.88 eV with increasing Co-content. PL spectra showed a strong green emission band thus confirming the formation of pure single ZnO phase. Magnetic studies showed that Co-doped ZnO NPs exhibited room temperature ferromagnetism (RTFM) and that the saturation magnetization attained a maximum value of 2.203 × 10^-3 emu/g for the highest Co-content. The antibacterial studies performed against a set of bacterial strains showed that the 2.0 wt% Co-doped ZnO NPs possessed a greater antibacterial effect.展开更多
文摘ZSM-5 zeolite with a hexagonal cubic morphology was synthesized by a hydrothermal method using Triton X-100, a nonionic surfactant. The samples prepared with and without the surfactant were characterized by X-ray diffraction(XRD), Fourier transform infrared spectroscopy, N2 adsorption, high resolution transmission electron microscopy(TEM), high resolution scanning electron mi-croscopy, energy dispersive X-ray analysis, and NH3 temperature-programmed desorption. The XRD patterns confirmed the formation of a pure ZSM-5 crystalline phase without secondary phases. TEM images revealed that the hexagonal cubes were made of peanut-shaped nanoparticles with voids.The catalytic activity of the zeolite samples was evaluated using the selective oxidation of benzyl alcohol with tertiary-butyl hydrogen peroxide as the oxidant at 90 °C. The surfactant-assisted prep-aration yielded a zeolite that gave a higher conversion than the one prepared in the absence of the surfactant. The catalyst was retrieved and reused four times without significant loss in activity and selectivity.
文摘Un-doped and Co-doped ZnO nanoparticles (NPs) with different weight ratios (0.5, 1.0, 1.5, and 2.0 wt% of Co) were synthesized by a facile and rapid microwave-assisted combustion method using urea as a fuel. The prepared NPs were characterized by X-ray diffraction (XRD), high resolution scanning electron microscopy (HR-SEM), energy dispersive X-ray analysis (EDX), diffuse reflectance spectroscopy (DRS), photoluminescence (PL) spectroscopy and vibrating sample magnetometry (VSM). XRD patterns refined by the Rietveld method indicated that Co-doped ZnO had a single pure phase with wurtzite structure suggesting that Co^2+ ions would occupy Zn^2+ ionic sites within the ZnO crystal lattice. Interestingly, the morphology was found to convert substantially from grains to nanoparticles with close-packed periodic array of hexagonal-like shape and then into randomly distributed spherical NPs with the variation of Co-content. The optical band gap estimated using DRS was found to be red-shifted from 3.22 eV for the un-doped ZnO NPs then decrease up to 2.88 eV with increasing Co-content. PL spectra showed a strong green emission band thus confirming the formation of pure single ZnO phase. Magnetic studies showed that Co-doped ZnO NPs exhibited room temperature ferromagnetism (RTFM) and that the saturation magnetization attained a maximum value of 2.203 × 10^-3 emu/g for the highest Co-content. The antibacterial studies performed against a set of bacterial strains showed that the 2.0 wt% Co-doped ZnO NPs possessed a greater antibacterial effect.