Thermoplastic elastomeric blends prepared from blending of (10%, 20%, 30%, 40% and 50 wt%) high density polyethylene(HDPE) and (10%, 20%, 30%, 40% and 50 wt%) ground rubber tire (TPV-R). The blends prepared contain (H...Thermoplastic elastomeric blends prepared from blending of (10%, 20%, 30%, 40% and 50 wt%) high density polyethylene(HDPE) and (10%, 20%, 30%, 40% and 50 wt%) ground rubber tire (TPV-R). The blends prepared contain (HDPE)/polybutadiene (TPV-V). The two blends were successfully prepared through a dynamic vulcanization process, involving dicumyl peroxide (3%) as vulcanizing agent. The data of the mechanical (tensile strength at yield, %elongation and young modulus) and rheological properties (shear stress, shear rate, viscosity, flow behavior index and activation energy of melt flow) of the TPV-V and TPV-R showed that there was comparable results between the two blends.展开更多
文摘Thermoplastic elastomeric blends prepared from blending of (10%, 20%, 30%, 40% and 50 wt%) high density polyethylene(HDPE) and (10%, 20%, 30%, 40% and 50 wt%) ground rubber tire (TPV-R). The blends prepared contain (HDPE)/polybutadiene (TPV-V). The two blends were successfully prepared through a dynamic vulcanization process, involving dicumyl peroxide (3%) as vulcanizing agent. The data of the mechanical (tensile strength at yield, %elongation and young modulus) and rheological properties (shear stress, shear rate, viscosity, flow behavior index and activation energy of melt flow) of the TPV-V and TPV-R showed that there was comparable results between the two blends.