Sintered zinc aluminum coating (SZAC) was prepared using zinc flakes, aluminum flakes and CrO 3 as main raw materials. The corrosion behavior of SZAC in 3.5%NaCl solution was studied by means of SEM, EDS, EIS and so o...Sintered zinc aluminum coating (SZAC) was prepared using zinc flakes, aluminum flakes and CrO 3 as main raw materials. The corrosion behavior of SZAC in 3.5%NaCl solution was studied by means of SEM, EDS, EIS and so on. Results indicate that aluminum corroded in advance of zinc to produce speculate or spherical substances, which attaches to SZAC and adds mass to it. Corrosion production passivates metal powders in SZAC, causes E corr of SZAC to increase gradually, and causes the arising of the third time constant in EIS, which corresponds to the insulation of corrosion production.展开更多
文摘Sintered zinc aluminum coating (SZAC) was prepared using zinc flakes, aluminum flakes and CrO 3 as main raw materials. The corrosion behavior of SZAC in 3.5%NaCl solution was studied by means of SEM, EDS, EIS and so on. Results indicate that aluminum corroded in advance of zinc to produce speculate or spherical substances, which attaches to SZAC and adds mass to it. Corrosion production passivates metal powders in SZAC, causes E corr of SZAC to increase gradually, and causes the arising of the third time constant in EIS, which corresponds to the insulation of corrosion production.